Final Magnetic Moment8.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.184 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.021 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCoO2 + Cr2CoO4 + LiCrO2 + Li2CrO4 |
Band Gap0.990 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 210.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 270.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 210.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 171.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 240.6 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 210.5 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 256.8 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 240.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 270.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 270.7 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 171.2 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 210.5 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 90.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 90.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 330.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 210.5 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 120.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 256.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 240.6 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 90.2 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 180.5 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 30.1 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 270.7 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 270.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 171.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 210.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 240.6 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 240.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 150.4 |
C (mp-66) | <1 1 0> | <0 0 1> | 150.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 90.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 240.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 360.9 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 256.8 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 240.6 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 171.2 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 360.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 150.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 120.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 30.1 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 270.7 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 330.8 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 171.2 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 330.8 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 270.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 210.5 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 270.7 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 180.5 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 256.8 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 210.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3(CoO2)4 (mp-763750) | 0.1661 | 0.140 | 3 |
Li3Cr4O8 (mp-771288) | 0.0839 | 0.034 | 3 |
Li3(CoO2)4 (mp-853206) | 0.1577 | 0.109 | 3 |
Li3(CoO2)4 (mvc-16807) | 0.1655 | 0.178 | 3 |
Li3(FeO2)4 (mp-769726) | 0.1193 | 0.034 | 3 |
Li3VCr3O8 (mp-771672) | 0.0878 | 0.038 | 4 |
Li3Cr2(FeO4)2 (mp-780017) | 0.0926 | 1.106 | 4 |
Li3VFe3O8 (mp-773273) | 0.0919 | 0.072 | 4 |
Li3CoNi3O8 (mp-765439) | 0.0901 | 0.097 | 4 |
Li3FeCo3O8 (mp-767943) | 0.1076 | 0.207 | 4 |
Fe7O8 (mp-705548) | 0.2661 | 0.099 | 2 |
Fe8O9 (mp-763787) | 0.2620 | 0.063 | 2 |
V8C7 (mp-542730) | 0.2468 | 0.007 | 2 |
Fe7O8 (mp-32939) | 0.2240 | 0.099 | 2 |
Fe7O8 (mp-715333) | 0.2696 | 0.064 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.5168 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eVCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv Co O |
Final Energy/Atom-6.7074 eV |
Corrected Energy-227.4844 eV
Uncorrected energy = -201.2224 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Composition-based energy adjustment (-1.999 eV/atom x 6.0 atoms) = -11.9940 eV
Composition-based energy adjustment (-1.638 eV/atom x 2.0 atoms) = -3.2760 eV
Corrected energy = -227.4844 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)