Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.141 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.311 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCoPO4 |
Band Gap2.707 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 338.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 338.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 188.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 188.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 263.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 301.2 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 168.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 301.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 150.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 338.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 188.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 338.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 188.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 188.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 338.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 196.0 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 225.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 188.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 338.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 263.6 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 301.2 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 338.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 338.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 188.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 338.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 338.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 263.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 37.7 |
BN (mp-984) | <1 1 0> | <0 0 1> | 263.6 |
BN (mp-984) | <1 1 1> | <0 0 1> | 301.2 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 263.6 |
LiNbO3 (mp-3731) | <1 1 1> | <0 0 1> | 263.6 |
Al (mp-134) | <1 1 0> | <0 0 1> | 338.9 |
Al (mp-134) | <1 1 1> | <1 0 1> | 196.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 301.2 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 225.9 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 1> | 147.0 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 263.6 |
LiTaO3 (mp-3666) | <1 1 1> | <0 0 1> | 263.6 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 150.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 263.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 301.2 |
C (mp-66) | <1 1 0> | <1 0 1> | 294.0 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 188.3 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 150.6 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 263.6 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 301.2 |
Ni (mp-23) | <1 0 0> | <1 0 1> | 98.0 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 150.6 |
Ni (mp-23) | <1 1 1> | <1 0 1> | 294.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2Ti2O5 (mp-779477) | 0.5197 | 0.026 | 3 |
Na2Ti2O5 (mp-760979) | 0.5655 | 0.031 | 3 |
Na2Ti2O5 (mp-779729) | 0.5604 | 0.035 | 3 |
Na2V2O5 (mp-764595) | 0.5223 | 0.138 | 3 |
MgSiO3 (mp-657338) | 0.5619 | 0.151 | 3 |
LiMnPO4 (mp-861693) | 0.2470 | 0.085 | 4 |
LiMnPO4 (mp-770763) | 0.3833 | 0.050 | 4 |
LiFePO4 (mp-766774) | 0.3156 | 0.310 | 4 |
LiFePO4 (mp-762555) | 0.3707 | 0.083 | 4 |
LiCoPO4 (mp-761753) | 0.4052 | 0.141 | 4 |
Bi19O30 (mp-773884) | 0.7494 | 0.050 | 2 |
Sr2AlCr2GaO7 (mvc-312) | 0.7142 | 0.186 | 5 |
Sr2YAlW2O7 (mvc-356) | 0.6989 | 0.551 | 5 |
Sr2YAlSn2O7 (mvc-10827) | 0.7253 | 0.246 | 5 |
NaLi2B(PO4)2 (mp-1020646) | 0.7102 | 0.000 | 5 |
Li2PWO4F (mp-25728) | 0.6302 | 0.352 | 5 |
KMg3AlSi3(O5F)2 (mp-684841) | 0.7219 | 0.230 | 6 |
Na4BeAlSi4ClO12 (mp-23151) | 0.6146 | 0.000 | 6 |
Explore more synthesis descriptions for materials of composition LiCoPO4.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co P O |
Final Energy/Atom-6.3606 eV |
Corrected Energy-393.6606 eV
-393.6606 eV = -356.1954 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 14.9920 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)