Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.847 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.027 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNiO + LiF |
Band Gap1.924 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group2/m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 135.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 168.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 219.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 160.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 227.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 143.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 303.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 33.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 236.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 168.8 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 278.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 168.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 160.3 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 194.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 219.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 135.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 167.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 244.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 329.1 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 168.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 16.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 75.9 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 92.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 16.9 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 118.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 177.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 270.0 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 211.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 109.7 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 329.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 42.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 75.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 126.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 244.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 270.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 244.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 177.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 244.7 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 211.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 42.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 211.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 312.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 236.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 75.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 33.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 236.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 118.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 84.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 84.4 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 295.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiTlO2 (mp-8179) | 0.0982 | 0.035 | 3 |
LiCo15O16 (mp-766743) | 0.1105 | 0.545 | 3 |
Y4AsSe3 (mp-38494) | 0.0870 | 0.000 | 3 |
LiDyS2 (mp-33667) | 0.1126 | 0.008 | 3 |
LiZrO2 (mp-755253) | 0.1168 | 0.056 | 3 |
Li4NiOF4 (mp-765887) | 0.0341 | 0.040 | 4 |
Mg14TiFeO16 (mp-1035726) | 0.0656 | 0.130 | 4 |
Mg30CoCO32 (mp-1098923) | 0.0639 | 0.169 | 4 |
Mg30MnVO32 (mp-1038167) | 0.0746 | 0.055 | 4 |
MnS (mp-850034) | 0.1951 | 0.000 | 2 |
KC (mp-1064300) | 0.1734 | 2.337 | 2 |
KC (mp-1064814) | 0.1546 | 2.337 | 2 |
CsI (mp-1078801) | 0.1880 | 0.003 | 2 |
MnO (mp-714882) | 0.1884 | 0.000 | 2 |
Hg (mp-982872) | 0.2348 | 0.020 | 1 |
Se (mp-7755) | 0.2205 | 0.181 | 1 |
K (mp-998881) | 0.2303 | 0.120 | 1 |
Te (mp-10654) | 0.2163 | 0.047 | 1 |
P (mp-53) | 0.2238 | 0.144 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv O F |
Final Energy/Atom-4.8358 eV |
Corrected Energy-141.1336 eV
-141.1336 eV = -135.4010 eV (uncorrected energy) - 4.3280 eV (MP Advanced Correction) - 1.4046 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)