Final Magnetic Moment17.037 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.817 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.105 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Fe3SbO8 + LiSbO3 + CuO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 324.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 324.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 194.8 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 270.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 244.4 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 305.5 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 305.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 64.9 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 194.8 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 270.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 270.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 183.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 324.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 194.8 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 259.7 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 210.3 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 324.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 194.8 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 270.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 259.7 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 194.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 244.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 324.6 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 183.3 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 129.8 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 64.9 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 305.5 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 259.7 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 324.6 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 324.6 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 183.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 259.7 |
C (mp-66) | <1 0 0> | <1 0 0> | 305.5 |
GdScO3 (mp-5690) | <1 1 1> | <0 1 0> | 210.3 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 183.3 |
BN (mp-984) | <0 0 1> | <1 0 0> | 244.4 |
BN (mp-984) | <1 0 0> | <1 0 0> | 305.5 |
BN (mp-984) | <1 1 1> | <1 0 0> | 305.5 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 324.6 |
Al (mp-134) | <1 0 0> | <1 0 0> | 244.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 324.6 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 183.3 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 129.8 |
C (mp-66) | <1 1 0> | <1 0 0> | 183.3 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 129.8 |
PbS (mp-21276) | <1 0 0> | <1 0 1> | 180.0 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 259.7 |
TbScO3 (mp-31119) | <1 1 1> | <0 1 0> | 210.3 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 259.7 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 259.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg7Al22O40 (mp-530826) | 0.3978 | 0.038 | 3 |
Ga23N5O27 (mp-530844) | 0.4036 | 0.067 | 3 |
Ga41N11O45 (mp-530841) | 0.3635 | 0.081 | 3 |
Ca(MoO2)2 (mvc-10002) | 0.3434 | 0.131 | 3 |
Ca(WO2)2 (mvc-10486) | 0.3974 | 0.389 | 3 |
Li6Fe3Sb3O16 (mp-771508) | 0.2941 | 0.073 | 4 |
Li6V3W3O16 (mp-771515) | 0.2935 | 0.065 | 4 |
Li4Co3Sb5O16 (mp-770677) | 0.2976 | 0.062 | 4 |
Li4Fe3Sb5O16 (mp-769870) | 0.3166 | 0.044 | 4 |
Li4Ni3Sb5O16 (mp-774248) | 0.3208 | 0.092 | 4 |
Al2S3 (mp-684676) | 0.5687 | 0.136 | 2 |
Fe41O56 (mp-762231) | 0.5492 | 0.210 | 2 |
Co23O32 (mp-705564) | 0.4863 | 0.068 | 2 |
Co29O40 (mp-705563) | 0.4864 | 0.120 | 2 |
Fe23O32 (mp-776135) | 0.4700 | 0.221 | 2 |
Li4Mn2Cr3Sb3O16 (mp-767785) | 0.2471 | 0.045 | 5 |
Li4Cr3Cu2Sb3O16 (mp-775356) | 0.1268 | 0.102 | 5 |
Li4V3Co2Sb3O16 (mp-770636) | 0.2320 | 0.055 | 5 |
Li4Mn2V3Sb3O16 (mp-765741) | 0.2333 | 0.029 | 5 |
Li4Fe3Co2Sb3O16 (mp-776141) | 0.2405 | 0.214 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Cu_pv Sb O |
Final Energy/Atom-5.8570 eV |
Corrected Energy-183.4328 eV
-183.4328 eV = -163.9972 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 8.1990 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)