Final Magnetic Moment1.794 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.181 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.291 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoO + LiF |
Band Gap0.044 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 356.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 174.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 139.3 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 122.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 165.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 113.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 113.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 339.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 304.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 34.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 243.8 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 173.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 78.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 200.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 252.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 174.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 287.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 278.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 182.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 165.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 252.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 339.5 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 217.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 78.4 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 287.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 269.9 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 278.6 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 174.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 217.6 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 182.8 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 260.3 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 43.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 156.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 252.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 322.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 139.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 174.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 252.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 78.4 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 306.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 130.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 34.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 243.8 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 173.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 78.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 304.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 313.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 78.4 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 86.8 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 95.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li4Ni7O11 (mp-768091) | 0.2728 | 0.031 | 3 |
Li7Ni9O16 (mp-768059) | 0.3052 | 0.021 | 3 |
LiNiO2 (mp-774102) | 0.2913 | 0.059 | 3 |
Li5Mn7O12 (mp-773337) | 0.2896 | 0.042 | 3 |
Li3MnO4 (mp-773369) | 0.3003 | 0.218 | 3 |
Li3Co4O4F3 (mp-764028) | 0.2477 | 0.130 | 4 |
Li5Nb2Co5O12 (mp-770965) | 0.2540 | 0.080 | 4 |
Li5Ni5(SnO6)2 (mp-773441) | 0.2654 | 0.015 | 4 |
Li5Co2O2F5 (mp-853153) | 0.0758 | 0.276 | 4 |
Li3TiMn4O8 (mp-771440) | 0.2470 | 0.062 | 4 |
Te2Au (mp-1662) | 0.3917 | 0.018 | 2 |
LiTe3 (mp-27466) | 0.4235 | 0.009 | 2 |
In2Se3 (mp-1068548) | 0.4774 | 0.530 | 2 |
In2Se3 (mp-20830) | 0.4920 | 0.530 | 2 |
Te2Au (mp-567525) | 0.4011 | 0.018 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.5742 | 0.139 | 5 |
Hg (mp-982872) | 0.6594 | 0.020 | 1 |
Sb (mp-632286) | 0.5584 | 0.059 | 1 |
Te (mp-570459) | 0.5792 | 0.044 | 1 |
Te (mp-10654) | 0.6983 | 0.047 | 1 |
Te (mp-105) | 0.5945 | 0.047 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co O F |
Final Energy/Atom-5.0760 eV |
Corrected Energy-56.7964 eV
Uncorrected energy = -50.7604 eV
Composition-based energy adjustment (-0.687 eV/atom x 2.0 atoms) = -1.3740 eV
Composition-based energy adjustment (-0.462 eV/atom x 3.0 atoms) = -1.3860 eV
Composition-based energy adjustment (-1.638 eV/atom x 2.0 atoms) = -3.2760 eV
Corrected energy = -56.7964 eV
|