Final Magnetic Moment9.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.573 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.042 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoO + CoF2 + LiF |
Band Gap2.794 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 -1> | 294.6 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 319.1 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 73.7 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 104.0 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 147.3 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 208.6 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 319.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 -1> | 294.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 319.1 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 221.0 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 127.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 221.0 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 319.1 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 319.1 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 191.4 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 191.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 255.3 |
Ag (mp-124) | <1 1 0> | <1 1 1> | 147.3 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 147.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 294.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 255.3 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 147.3 |
GaSe (mp-1943) | <0 0 1> | <1 0 -1> | 294.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 294.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 147.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 207.9 |
BN (mp-984) | <0 0 1> | <1 0 0> | 319.1 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 294.6 |
BN (mp-984) | <1 0 1> | <1 0 -1> | 221.0 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 207.9 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 191.4 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 0> | 319.1 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 191.4 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 104.0 |
Al (mp-134) | <1 0 0> | <1 1 1> | 147.3 |
Al (mp-134) | <1 1 0> | <0 1 0> | 207.9 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 -1> | 221.0 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 319.1 |
TiO2 (mp-2657) | <1 0 0> | <1 0 -1> | 221.0 |
TeO2 (mp-2125) | <0 0 1> | <1 0 -1> | 294.6 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 207.9 |
TeO2 (mp-2125) | <1 1 0> | <1 0 -1> | 294.6 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 255.3 |
Mg (mp-153) | <1 1 1> | <1 0 -1> | 147.3 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 191.4 |
Fe3O4 (mp-19306) | <1 0 0> | <1 1 1> | 147.3 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 -1> | 127.4 |
MgO (mp-1265) | <1 0 0> | <1 0 -1> | 73.7 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 63.8 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 319.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ga2NiO4 (mp-698638) | 0.1088 | 0.011 | 3 |
Ga2CoO4 (mp-698589) | 0.0922 | 0.247 | 3 |
Mg(GaO2)2 (mp-35712) | 0.1131 | 0.018 | 3 |
Mg(GaO2)2 (mp-530121) | 0.1092 | 0.020 | 3 |
Mg(GaO2)2 (mp-530303) | 0.1018 | 0.023 | 3 |
LiZn2Fe9O16 (mp-773576) | 0.1078 | 0.077 | 4 |
Li4V2OF7 (mp-765046) | 0.1198 | 0.054 | 4 |
Li3Co3OF7 (mp-765518) | 0.0977 | 0.042 | 4 |
Li3Ni3OF7 (mp-765792) | 0.1198 | 0.032 | 4 |
Li3Co3OF7 (mp-764203) | 0.1213 | 0.040 | 4 |
Fe3O4 (mp-715491) | 0.1783 | 0.017 | 2 |
Fe3O4 (mp-542433) | 0.1995 | 0.075 | 2 |
Fe3O4 (mp-650112) | 0.1786 | 0.060 | 2 |
Fe3O4 (mp-31770) | 0.1952 | 0.017 | 2 |
Fe3O4 (mp-715558) | 0.2029 | 0.785 | 2 |
Li4Ti3Cr3(SnO8)2 (mp-776780) | 0.2162 | 0.138 | 5 |
Li14Mn22Cr3Cu3O56 (mp-735790) | 0.2254 | 0.014 | 5 |
Li4Ti3Cr3(WO8)2 (mp-773537) | 0.2080 | 0.046 | 5 |
Li4Cr3Fe3(TeO8)2 (mp-773518) | 0.2043 | 1.173 | 5 |
Li4Cr3Fe3(SbO8)2 (mp-771925) | 0.2223 | 0.871 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.7212 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.7086 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.7148 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.7153 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.7200 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co O F |
Final Energy/Atom-5.1167 eV |
Corrected Energy-155.9173 eV
-155.9173 eV = -143.2688 eV (uncorrected energy) - 11.2440 eV (MP Advanced Correction) - 1.4046 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)