material

MnCoO4

ID:

mp-752945


Material Details

Final Magnetic Moment
0.371 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-1.438 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.025 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.34 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CoO2 + MnO2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P2/m [10]
Hall
-P 2y
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiO2 (mp-6930) <1 1 1> <0 1 0> 0.001 211.5
CaF2 (mp-2741) <1 1 0> <0 1 0> 0.001 258.5
Ge (mp-32) <1 1 0> <0 1 0> 0.001 47.0
GaP (mp-2490) <1 1 0> <0 1 0> 0.001 258.5
GaAs (mp-2534) <1 1 0> <0 1 0> 0.001 47.0
InSb (mp-20012) <1 1 0> <0 1 0> 0.002 188.0
DyScO3 (mp-31120) <0 0 1> <0 1 0> 0.002 94.0
ZnSe (mp-1190) <1 1 0> <0 1 0> 0.002 47.0
CdTe (mp-406) <1 1 0> <0 1 0> 0.002 188.0
MgAl2O4 (mp-3536) <1 1 0> <0 1 0> 0.003 94.0
CdWO4 (mp-19387) <1 0 1> <0 1 0> 0.003 352.5
NdGaO3 (mp-3196) <0 1 0> <0 1 0> 0.004 258.5
MgAl2O4 (mp-3536) <1 0 0> <1 0 -1> 0.004 66.6
Ni (mp-23) <1 1 0> <0 1 0> 0.004 70.5
CeO2 (mp-20194) <1 0 0> <1 0 -1> 0.004 266.5
TbScO3 (mp-31119) <0 0 1> <0 1 0> 0.005 94.0
MgO (mp-1265) <1 1 1> <0 0 1> 0.005 187.2
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.005 187.2
Si (mp-149) <1 0 0> <1 0 -1> 0.005 266.5
LiF (mp-1138) <1 0 0> <1 1 1> 0.006 33.3
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.006 43.2
GaN (mp-804) <0 0 1> <0 0 1> 0.007 115.2
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.007 187.2
SiO2 (mp-6930) <1 0 1> <0 1 0> 0.007 70.5
MgAl2O4 (mp-3536) <1 1 1> <0 0 1> 0.008 115.2
TiO2 (mp-2657) <1 0 1> <0 1 0> 0.008 235.0
CdWO4 (mp-19387) <0 1 1> <0 1 0> 0.009 164.5
MgF2 (mp-1249) <1 1 0> <0 1 0> 0.009 188.0
BN (mp-984) <0 0 1> <0 0 1> 0.009 43.2
Si (mp-149) <1 1 0> <0 1 0> 0.009 258.5
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.009 187.2
GdScO3 (mp-5690) <1 0 0> <0 1 0> 0.009 47.0
CeO2 (mp-20194) <1 1 0> <0 1 0> 0.009 258.5
LiF (mp-1138) <1 1 1> <0 0 1> 0.009 28.8
WSe2 (mp-1821) <1 0 0> <0 1 1> 0.010 248.0
CdWO4 (mp-19387) <1 1 0> <0 1 0> 0.010 164.5
LiGaO2 (mp-5854) <1 1 1> <0 1 0> 0.010 282.0
YAlO3 (mp-3792) <1 1 1> <0 1 1> 0.010 248.0
NdGaO3 (mp-3196) <0 1 1> <0 1 0> 0.011 258.5
CdS (mp-672) <1 0 0> <0 1 0> 0.012 258.5
LiGaO2 (mp-5854) <1 0 1> <1 0 -1> 0.012 133.2
CdWO4 (mp-19387) <1 1 1> <0 1 0> 0.013 211.5
MoS2 (mp-1434) <1 0 0> <0 1 1> 0.013 137.8
NdGaO3 (mp-3196) <0 0 1> <0 1 0> 0.015 94.0
KP(HO2)2 (mp-23959) <0 1 1> <0 1 0> 0.015 211.5
TbScO3 (mp-31119) <1 0 0> <0 1 0> 0.016 47.0
Al2O3 (mp-1143) <1 0 1> <0 1 0> 0.017 258.5
NaCl (mp-22862) <1 1 0> <0 1 0> 0.017 47.0
C (mp-48) <1 0 0> <0 1 0> 0.017 117.5
CdS (mp-672) <1 0 1> <0 1 1> 0.017 192.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Mn13Fe3O32 (mp-771188) 0.0919 0.080 3
Mn3CoO8 (mp-772359) 0.0866 0.027 3
MnCo3O8 (mp-773602) 0.0776 0.021 3
CrCo3O8 (mp-765865) 0.0884 0.107 3
Mn5FeO12 (mp-777021) 0.0719 0.139 3
Ti2Mn3Cr3O16 (mp-771540) 0.4898 0.084 4
Ti3Mn3Cr2O16 (mp-770915) 0.4998 0.098 4
Mn3Cr3(WO8)2 (mp-778921) 0.4880 0.103 4
LiV3(OF3)2 (mp-766156) 0.4625 0.082 4
Mn3Cr3(TeO8)2 (mp-772458) 0.4913 0.082 4
TiO2 (mvc-11912) 0.1199 0.179 2
MnO2 (mvc-11542) 0.1538 0.014 2
CoO2 (mp-559382) 0.1538 0.008 2
CoO2 (mp-715480) 0.1002 0.008 2
MnO2 (mp-715446) 0.1330 0.033 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Mn: 3.9 eV
Co: 3.32 eV
Pseudopotentials
VASP PAW: Mn_pv Co O
Final Energy/Atom
-6.4198 eV
Corrected Energy
-44.5726 eV
Uncorrected energy = -38.5186 eV Composition-based energy adjustment (-0.687 eV/atom x 4.0 atoms) = -2.7480 eV Composition-based energy adjustment (-1.668 eV/atom x 1.0 atoms) = -1.6680 eV Composition-based energy adjustment (-1.638 eV/atom x 1.0 atoms) = -1.6380 eV Corrected energy = -44.5726 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)