Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.985 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.062 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.76 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2VOF4 |
Band Gap2.632 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPna21 [33] |
HallP 2c 2n |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 260.9 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 0> | 260.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 117.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 353.1 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 196.0 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 286.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 117.7 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 209.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 117.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 235.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 196.0 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 173.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 156.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 130.7 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 52.2 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 209.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 196.1 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 173.9 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 196.0 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 196.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 196.1 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 235.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 52.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 278.1 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 209.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 196.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 274.6 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 353.1 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 196.1 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 159.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 196.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 239.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 156.9 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 139.1 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 69.5 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 261.2 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 173.9 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 319.3 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 196.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 274.6 |
BN (mp-984) | <0 0 1> | <0 1 0> | 104.5 |
BN (mp-984) | <1 0 0> | <0 1 0> | 156.7 |
LiNbO3 (mp-3731) | <1 1 0> | <1 1 0> | 260.9 |
LiNbO3 (mp-3731) | <1 1 1> | <1 1 0> | 260.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 104.5 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 52.2 |
MoS2 (mp-1434) | <1 0 0> | <0 1 0> | 209.0 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 117.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 196.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 196.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V3SnO8 (mp-778681) | 0.6763 | 0.069 | 3 |
Nb2SbO6 (mp-755840) | 0.6574 | 0.069 | 3 |
Ag2W2O7 (mp-32537) | 0.6393 | 0.028 | 3 |
Nb2CuO6 (mp-4643) | 0.7303 | 0.043 | 3 |
Nb2SnO6 (mp-3324) | 0.7369 | 0.000 | 3 |
Li2VOF4 (mp-766764) | 0.2448 | 0.064 | 4 |
Li2VO2F3 (mp-772563) | 0.5312 | 0.088 | 4 |
Ca2Nb2SbO8 (mvc-87) | 0.5818 | 0.179 | 4 |
Ca2Nb2CuO8 (mvc-89) | 0.6307 | 0.113 | 4 |
Ca2Ta2CuO8 (mvc-2427) | 0.5840 | 0.123 | 4 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O F |
Final Energy/Atom-5.6287 eV |
Corrected Energy-197.0575 eV
Uncorrected energy = -180.1175 eV
Composition-based energy adjustment (-0.687 eV/atom x 4.0 atoms) = -2.7480 eV
Composition-based energy adjustment (-0.462 eV/atom x 16.0 atoms) = -7.3920 eV
Composition-based energy adjustment (-1.700 eV/atom x 4.0 atoms) = -6.8000 eV
Corrected energy = -197.0575 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)