Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.491 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.066 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.34 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFePO4 |
Band Gap3.532 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 1> | 170.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 126.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 108.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 252.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 189.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 63.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 108.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 189.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 217.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 189.4 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 315.6 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 189.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 189.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 108.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 287.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 245.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 189.4 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 252.5 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 287.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 189.4 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 63.1 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 108.7 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 0> | 217.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 253.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 189.4 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 315.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 315.6 |
BN (mp-984) | <1 1 0> | <0 1 0> | 229.6 |
BN (mp-984) | <1 1 1> | <0 1 0> | 229.6 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 63.1 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 108.7 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 189.4 |
TbScO3 (mp-31119) | <1 1 1> | <1 0 0> | 217.3 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 229.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 315.6 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 287.0 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 252.5 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 189.4 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 189.4 |
BaTiO3 (mp-5986) | <1 1 1> | <0 1 0> | 57.4 |
Al (mp-134) | <1 0 0> | <1 1 0> | 245.8 |
Al (mp-134) | <1 1 0> | <0 0 1> | 189.4 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 63.1 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 315.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 252.5 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 172.2 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 315.6 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 315.6 |
SiC (mp-11714) | <1 0 0> | <1 1 0> | 122.9 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 108.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn3(PO4)2 (mp-699908) | 0.6203 | 0.010 | 3 |
Na6Ti2O7 (mp-850957) | 0.6068 | 0.040 | 3 |
Li4SiO4 (mp-685863) | 0.6054 | 0.058 | 3 |
Na4CoO4 (mp-764107) | 0.5762 | 0.088 | 3 |
Cd3(AsO4)2 (mp-13602) | 0.5155 | 0.000 | 3 |
LiNiPO4 (mp-765391) | 0.2291 | 0.253 | 4 |
LiCuPO4 (mp-758990) | 0.2528 | 0.072 | 4 |
LiMnPO4 (mp-861465) | 0.3105 | 0.063 | 4 |
LiCoPO4 (mp-772438) | 0.1206 | 0.194 | 4 |
LiCrPO4 (mp-761398) | 0.2619 | 0.045 | 4 |
LiMnPO4F (mp-762683) | 0.7059 | 0.211 | 5 |
Sr2AlCr2GaO7 (mvc-312) | 0.6433 | 0.186 | 5 |
Sr2AlGaCo2O7 (mvc-3397) | 0.7028 | 0.319 | 5 |
Na3Li2Al(SiO4)2 (mp-1020163) | 0.7034 | 0.000 | 5 |
Li2PWO4F (mp-25728) | 0.6636 | 0.352 | 5 |
Na2LiCaVP2O9 (mp-763838) | 0.6836 | 0.111 | 6 |
Na2SrLiVP2O9 (mp-763837) | 0.6890 | 0.101 | 6 |
Explore more synthesis descriptions for materials of composition LiFePO4.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P O |
Final Energy/Atom-6.7824 eV |
Corrected Energy-424.1516 eV
-424.1516 eV = -379.8144 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 21.8640 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)