Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.438 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.045 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVHO2 + LiVPHO5 + LiMnPO4 + Li3PO4 + H2O |
Band Gap2.035 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 175.3 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 -1> | 278.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 221.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 146.1 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 78.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 159.3 |
AlN (mp-661) | <1 1 0> | <1 -1 0> | 197.1 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 199.2 |
CeO2 (mp-20194) | <1 0 0> | <1 1 -1> | 271.7 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 166.4 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 199.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 358.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 278.8 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 199.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 204.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 321.4 |
GaN (mp-804) | <1 1 0> | <1 -1 0> | 197.1 |
GaN (mp-804) | <1 1 1> | <0 1 -1> | 278.5 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 345.7 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 192.1 |
SiO2 (mp-6930) | <1 0 1> | <1 -1 1> | 174.6 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 192.1 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 262.9 |
KCl (mp-23193) | <1 0 0> | <1 -1 0> | 295.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 -1> | 159.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 166.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 159.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 278.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 313.7 |
DyScO3 (mp-31120) | <1 1 1> | <1 -1 -1> | 281.7 |
InAs (mp-20305) | <1 0 0> | <1 -1 0> | 344.9 |
InAs (mp-20305) | <1 1 1> | <1 -1 -1> | 338.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 358.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 278.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 -1> | 278.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 175.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 235.3 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 268.9 |
CdS (mp-672) | <1 0 0> | <0 1 -1> | 198.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 262.9 |
CdS (mp-672) | <1 0 1> | <1 -1 -1> | 225.4 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 199.2 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 321.4 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 235.3 |
LiF (mp-1138) | <1 1 1> | <0 1 -1> | 278.5 |
Te2W (mp-22693) | <0 0 1> | <1 -1 1> | 174.6 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 230.5 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 204.5 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 262.9 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 159.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe4P2O9 (mp-637226) | 0.7158 | 0.013 | 3 |
Mn4P2O9 (mp-770499) | 0.6923 | 0.015 | 3 |
Cr4P2O9 (mp-773396) | 0.7363 | 0.059 | 3 |
V3(PO4)2 (mp-771054) | 0.7297 | 0.051 | 3 |
Mg7P2(HO2)8 (mp-699232) | 0.5988 | 0.000 | 4 |
Li3Bi(PO4)2 (mp-759624) | 0.6241 | 0.071 | 4 |
Mg2PHO5 (mp-23740) | 0.5654 | 0.000 | 4 |
Li2VPO5 (mp-778299) | 0.5653 | 0.089 | 4 |
CdH4NCl3 (mp-24356) | 0.5841 | 0.000 | 4 |
LiNiPHO5 (mp-768033) | 0.4456 | 0.062 | 5 |
LiCrPHO5 (mp-765883) | 0.4936 | 0.000 | 5 |
LiMnPHO5 (mp-769993) | 0.4751 | 0.000 | 5 |
LiAlPHO5 (mp-644409) | 0.4961 | 0.001 | 5 |
Li2MnPHO5 (mp-776527) | 0.4866 | 0.055 | 5 |
Li2MnVP2(HO5)2 (mp-849445) | 0.5059 | 0.015 | 6 |
Li2MnVP2(HO5)2 (mp-849423) | 0.5064 | 0.027 | 6 |
Li3VFeP2(HO5)2 (mp-765312) | 0.1299 | 0.139 | 6 |
Li2MnVP2(HO5)2 (mp-849682) | 0.4842 | 0.031 | 6 |
Li2MnVP2(HO5)2 (mp-776718) | 0.5095 | 0.035 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv V_pv P H O |
Final Energy/Atom-6.6686 eV |
Corrected Energy-274.1774 eV
-274.1774 eV = -253.4059 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction) - 6.7257 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)