Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.600 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.068 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Si2O5 + CuO + SiO2 |
Band Gap0.418 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 -1 1> | 179.5 |
AlN (mp-661) | <1 0 0> | <1 -1 -1> | 248.9 |
AlN (mp-661) | <1 0 1> | <1 -1 -1> | 248.9 |
AlN (mp-661) | <1 1 0> | <1 -1 1> | 269.2 |
AlN (mp-661) | <1 1 1> | <1 1 -1> | 201.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 260.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 307.7 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 260.9 |
GaAs (mp-2534) | <1 1 0> | <1 -1 0> | 139.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 205.1 |
GaN (mp-804) | <1 0 0> | <1 -1 1> | 269.2 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 212.1 |
GaN (mp-804) | <1 1 0> | <1 1 -1> | 201.3 |
SiO2 (mp-6930) | <1 0 0> | <1 -1 1> | 269.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 256.4 |
Al (mp-134) | <1 1 0> | <1 -1 -1> | 248.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 307.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 296.3 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 326.2 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 307.7 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 -1> | 278.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 -1 0> | 278.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 -1 0> | 139.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 282.8 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 307.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 256.4 |
ZnSe (mp-1190) | <1 1 0> | <1 -1 0> | 139.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 -1 -1> | 248.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 326.2 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 257.1 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 237.1 |
SiC (mp-7631) | <0 0 1> | <1 1 0> | 206.9 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 258.9 |
LiF (mp-1138) | <1 1 1> | <1 -1 0> | 208.7 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 307.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 256.4 |
Te2W (mp-22693) | <0 1 0> | <1 -1 0> | 208.7 |
Te2W (mp-22693) | <0 1 1> | <1 -1 1> | 179.5 |
MgO (mp-1265) | <1 0 0> | <1 -1 -1> | 248.9 |
MgO (mp-1265) | <1 1 0> | <1 -1 0> | 278.3 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 206.9 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 258.9 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 326.2 |
TiO2 (mp-2657) | <1 0 1> | <0 1 -1> | 278.2 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 256.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 307.7 |
Ag (mp-124) | <1 0 0> | <1 1 1> | 257.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 307.7 |
Ag (mp-124) | <1 1 1> | <1 -1 0> | 208.7 |
C (mp-66) | <1 1 0> | <1 0 0> | 195.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2V2O5 (mp-780306) | 0.6490 | 0.141 | 3 |
Cu4(PO4)3 (mp-26742) | 0.6653 | 0.028 | 3 |
V2(CuO2)5 (mp-559440) | 0.6604 | 0.033 | 3 |
Cr3(PO4)2 (mp-579247) | 0.6820 | 0.089 | 3 |
V2Cu3O8 (mp-600273) | 0.6853 | 0.018 | 3 |
Li2Cu4Si4O13 (mp-766013) | 0.5068 | 0.125 | 4 |
LiFePO4 (mp-765963) | 0.5345 | 0.481 | 4 |
Li2Fe2Si4O11 (mp-761735) | 0.5720 | 0.182 | 4 |
Li2Cr2Si4O11 (mp-761645) | 0.1983 | 0.177 | 4 |
Li2Mg2Si4O11 (mp-561336) | 0.5676 | 0.015 | 4 |
Na6Al4Fe(Si4O13)2 (mp-39647) | 0.4871 | 0.043 | 5 |
Li7CuAs4ClO14 (mp-769204) | 0.6730 | 0.074 | 5 |
Na6Al4Fe(Si4O13)2 (mp-42298) | 0.5287 | 0.000 | 5 |
Na6Al4Fe(Si4O13)2 (mp-705484) | 0.5260 | 0.033 | 5 |
Na6Al4Fe(Si4O13)2 (mp-698697) | 0.4773 | 0.043 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Cu_pv Si O |
Final Energy/Atom-6.8327 eV |
Corrected Energy-275.0912 eV
-275.0912 eV = -259.6409 eV (uncorrected energy) - 15.4504 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)