Final Magnetic Moment37.125 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.903 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAl2FeO4 + FeO + Fe2O3 |
Band Gap2.209 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 236.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 235.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 235.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 177.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 135.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 112.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 224.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 235.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 235.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 295.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 295.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 59.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 118.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 112.2 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 117.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 177.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 118.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 177.2 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 118.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 59.1 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 295.3 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 295.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 236.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 295.3 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 224.5 |
Al (mp-134) | <1 1 0> | <0 0 1> | 118.1 |
Al (mp-134) | <1 1 1> | <1 0 0> | 112.2 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 177.2 |
TeO2 (mp-2125) | <1 0 1> | <1 0 -1> | 235.5 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 295.3 |
C (mp-66) | <1 1 1> | <0 0 1> | 177.2 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 177.2 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 193.4 |
TiO2 (mp-2657) | <1 1 0> | <1 0 -1> | 117.8 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 -1> | 235.5 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 112.2 |
C (mp-66) | <1 1 0> | <0 0 1> | 177.2 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 224.5 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 295.3 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 177.2 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 224.5 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 295.3 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 -1> | 235.5 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 112.2 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 295.3 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 177.2 |
MoSe2 (mp-1634) | <1 1 1> | <0 0 1> | 177.2 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 236.2 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 177.2 |
Ga2O3 (mp-886) | <1 1 0> | <0 0 1> | 295.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
EuY2O4 (mp-754557) | 0.0787 | 0.012 | 3 |
Y(NiO2)2 (mvc-11636) | 0.0670 | 0.132 | 3 |
Y(CuO2)2 (mvc-4130) | 0.0729 | 0.300 | 3 |
SrSm2O4 (mp-754942) | 0.0751 | 0.020 | 3 |
Ca(MoO2)2 (mvc-4908) | 0.0791 | 0.000 | 3 |
Li2Cr3FeO8 (mp-774415) | 0.1183 | 0.605 | 4 |
Li2CoNi3O8 (mp-761777) | 0.1200 | 0.016 | 4 |
LiCoNiO4 (mp-776511) | 0.0871 | 0.000 | 4 |
Li2Co3NiO8 (mp-761738) | 0.0913 | 0.226 | 4 |
Li2MnFe3O8 (mp-775094) | 0.0948 | 0.095 | 4 |
Co3O4 (mp-559191) | 0.1270 | 0.010 | 2 |
In3S4 (mp-556597) | 0.2568 | 0.042 | 2 |
Co3O4 (mp-18748) | 0.1014 | 0.010 | 2 |
Ni3S4 (mp-1050) | 0.3014 | 0.000 | 2 |
Sn3N4 (mp-16031) | 0.2764 | 0.000 | 2 |
Li4Cr2Fe3Co3O16 (mp-775698) | 0.4385 | 0.894 | 5 |
Li4Mn2Fe3Co3O16 (mp-761441) | 0.4410 | 0.079 | 5 |
Li14Mn22Cr3Cu3O56 (mp-735790) | 0.4138 | 0.019 | 5 |
Li4Mn3Cr3(CuO8)2 (mp-765456) | 0.4202 | 0.080 | 5 |
Li4Cr3Cu3(SbO8)2 (mp-783908) | 0.4439 | 0.040 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Al Fe_pv O |
Final Energy/Atom-7.2546 eV |
Corrected Energy-453.3292 eV
-453.3292 eV = -406.2589 eV (uncorrected energy) - 24.5970 eV (MP Advanced Correction) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)