Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.146 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.030 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNiO + LiBO2 |
Band Gap3.274 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 138.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 324.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 185.1 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 140.6 |
GaAs (mp-2534) | <1 1 1> | <0 1 1> | 281.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 231.4 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 277.7 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 262.6 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 317.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 138.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 231.4 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 87.5 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 324.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 231.4 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 262.6 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 262.6 |
ZnSe (mp-1190) | <1 1 1> | <0 1 1> | 281.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 324.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 204.6 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 264.5 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 231.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 277.7 |
BN (mp-984) | <0 0 1> | <1 0 0> | 87.5 |
BN (mp-984) | <1 0 0> | <0 1 1> | 210.9 |
BN (mp-984) | <1 0 1> | <1 0 0> | 262.6 |
BN (mp-984) | <1 1 0> | <0 0 1> | 138.9 |
BN (mp-984) | <1 1 1> | <0 0 1> | 138.9 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 102.3 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 262.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 264.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 138.9 |
Al (mp-134) | <1 1 0> | <1 1 0> | 204.6 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 211.6 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 200.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 262.6 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 317.4 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 231.4 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 262.6 |
MgO (mp-1265) | <1 1 1> | <0 1 1> | 281.1 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 264.5 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 211.6 |
TiO2 (mp-2657) | <1 0 1> | <0 1 1> | 281.1 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 175.1 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 231.4 |
C (mp-66) | <1 0 0> | <1 1 0> | 102.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 324.0 |
C (mp-66) | <1 1 1> | <1 0 0> | 87.5 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 175.1 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 185.1 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 231.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3MnF5 (mp-763332) | 0.6931 | 0.083 | 3 |
Li3BO3 (mp-27275) | 0.6490 | 0.000 | 3 |
Na3CoO3 (mp-777919) | 0.4781 | 0.127 | 3 |
LiMnBO3 (mp-849500) | 0.2367 | 0.000 | 4 |
LiCuBO3 (mp-753471) | 0.2189 | 0.089 | 4 |
LiMnBO3 (mp-850971) | 0.2670 | 0.006 | 4 |
LiFeBO3 (mp-777711) | 0.2688 | 0.000 | 4 |
LiFeBO3 (mp-783910) | 0.2631 | 0.652 | 4 |
Li8MnFe7(BO3)8 (mp-850743) | 0.2423 | 0.017 | 5 |
Li4MnFe3(BO3)4 (mp-778654) | 0.2348 | 0.023 | 5 |
Li8Mn3Fe5(BO3)8 (mp-778883) | 0.2266 | 0.015 | 5 |
Li8Mn5Fe3(BO3)8 (mp-780292) | 0.2349 | 0.011 | 5 |
Li8MnFe7(BO3)8 (mp-779381) | 0.2446 | 0.018 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv B O |
Final Energy/Atom-6.3030 eV |
Corrected Energy-168.3561 eV
-168.3561 eV = -151.2727 eV (uncorrected energy) - 8.6560 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)