Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.631 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.063 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaI2 + BaI2 |
Band Gap3.601 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP321 [150] |
HallP 3 2" |
Point Group32 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 171.3 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 204.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 171.3 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 102.3 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 102.3 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 102.3 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 204.6 |
C (mp-66) | <1 0 0> | <1 0 0> | 102.3 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 171.3 |
CdWO4 (mp-19387) | <1 0 1> | <1 1 0> | 177.2 |
CdWO4 (mp-19387) | <1 1 1> | <1 0 0> | 102.3 |
Ge (mp-32) | <1 1 1> | <0 0 1> | 171.3 |
Al2O3 (mp-1143) | <1 0 1> | <1 0 0> | 204.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SrCa2I6 (mp-752695) | 0.1739 | 0.047 | 3 |
BaSr2I6 (mp-752439) | 0.1536 | 0.027 | 3 |
BaCa2I6 (mp-766352) | 0.2133 | 0.047 | 3 |
SrCaI4 (mp-754885) | 0.2218 | 0.046 | 3 |
BaSr2I6 (mp-772876) | 0.2126 | 0.017 | 3 |
LiGaPdF6 (mp-9245) | 0.3256 | 0.012 | 4 |
LiV2OF5 (mp-765917) | 0.4037 | 0.097 | 4 |
LiMnFeF6 (mp-566418) | 0.3785 | 0.000 | 4 |
LiCdCoF6 (mp-558057) | 0.3767 | 0.001 | 4 |
LiTiMnF6 (mp-556715) | 0.3502 | 0.025 | 4 |
Mn2N (mp-9981) | 0.3092 | 0.000 | 2 |
Fe2N (mp-21476) | 0.3296 | 0.057 | 2 |
Co2C (mp-22488) | 0.2906 | 0.108 | 2 |
CaCl2 (mp-571642) | 0.3242 | 0.001 | 2 |
YbBr2 (mp-571232) | 0.2848 | 0.001 | 2 |
Li4ZrNb(TeO6)2 (mp-756177) | 0.6126 | 0.058 | 5 |
LaMnZnFeO6 (mvc-8951) | 0.6428 | 0.178 | 5 |
LaZnFeSbO6 (mvc-9031) | 0.6688 | 0.099 | 5 |
LaZnCrWO6 (mvc-9890) | 0.6940 | 0.166 | 5 |
LaZnFeCoO6 (mvc-9020) | 0.6758 | 0.120 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Ca_sv I |
Final Energy/Atom-3.3058 eV |
Corrected Energy-89.2570 eV
-89.2570 eV = -89.2570 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)