Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.706 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.041 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaI2 + BaI2 |
Band Gap3.841 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcn [60] |
Hall-P 2n 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 313.2 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 196.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 234.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 234.9 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 196.9 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 234.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 234.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 234.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 234.9 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 234.9 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 313.2 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 196.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 313.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 313.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 313.2 |
Al (mp-134) | <1 0 0> | <0 1 0> | 196.9 |
Al (mp-134) | <1 1 0> | <0 0 1> | 234.9 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 313.2 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 313.2 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 313.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 313.2 |
Fe3O4 (mp-19306) | <1 1 0> | <0 1 0> | 196.9 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 234.9 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 313.2 |
InP (mp-20351) | <1 1 0> | <0 1 0> | 196.9 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 234.9 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 313.2 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 234.9 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 234.9 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 156.6 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 156.6 |
Au (mp-81) | <1 1 0> | <0 1 0> | 196.9 |
C (mp-48) | <1 1 1> | <0 0 1> | 234.9 |
NaCl (mp-22862) | <1 0 0> | <0 1 0> | 196.9 |
NaCl (mp-22862) | <1 1 0> | <0 0 1> | 234.9 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 234.9 |
ZrO2 (mp-2858) | <1 0 1> | <0 0 1> | 313.2 |
YAlO3 (mp-3792) | <1 1 1> | <0 0 1> | 313.2 |
MgAl2O4 (mp-3536) | <1 1 0> | <0 1 0> | 196.9 |
Cu (mp-30) | <1 0 0> | <0 1 0> | 196.9 |
GaTe (mp-542812) | <1 0 1> | <0 1 0> | 196.9 |
Ge (mp-32) | <1 0 0> | <0 1 0> | 196.9 |
Ge (mp-32) | <1 1 0> | <0 0 1> | 234.9 |
Ge (mp-32) | <1 1 1> | <0 0 1> | 234.9 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 234.9 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 313.2 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 156.6 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 78.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnOF (mp-763969) | 0.2846 | 0.075 | 3 |
Mn6OF11 (mp-764092) | 0.2949 | 0.031 | 3 |
MnOF (mp-851034) | 0.2682 | 0.312 | 3 |
NiWO4 (mp-25094) | 0.2875 | 0.000 | 3 |
CoWO4 (mp-19092) | 0.2924 | 0.000 | 3 |
Mn3Cr2Sb3O16 (mp-775041) | 0.3111 | 0.324 | 4 |
V3Cr2Sb3O16 (mp-778794) | 0.2991 | 0.127 | 4 |
Mn3Fe3(CoO8)2 (mp-770195) | 0.3156 | 0.139 | 4 |
AlSn(WO4)2 (mvc-732) | 0.3046 | 0.109 | 4 |
TaAl(WO4)2 (mvc-640) | 0.3113 | 0.088 | 4 |
Rb2O (mp-755459) | 0.3417 | 0.018 | 2 |
CrO2 (mvc-5834) | 0.3323 | 0.071 | 2 |
TiO2 (mvc-11500) | 0.3365 | 0.074 | 2 |
CeSe2 (mp-1080851) | 0.3062 | 0.127 | 2 |
VO2 (mvc-12071) | 0.3464 | 0.059 | 2 |
Li4ZrNb(TeO6)2 (mp-756177) | 0.7140 | 0.058 | 5 |
LaZnCrWO6 (mvc-9890) | 0.7055 | 0.175 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Ca_sv I |
Final Energy/Atom-3.3704 eV |
Corrected Energy-130.4300 eV
Uncorrected energy = -121.3340 eV
Composition-based energy adjustment (-0.379 eV/atom x 24.0 atoms) = -9.0960 eV
Corrected energy = -130.4300 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)