Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.645 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.047 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaI2 + BaI2 |
Band Gap3.689 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcn [60] |
Hall-P 2n 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LiF (mp-1138) | <1 0 0> | <0 0 1> | 305.9 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 183.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 305.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 244.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 244.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 61.2 |
Al (mp-134) | <1 1 0> | <0 0 1> | 183.5 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 183.5 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 244.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 244.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 244.7 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 305.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 244.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 305.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 305.9 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 244.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 244.7 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 305.9 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 305.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 183.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 61.2 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 305.9 |
C (mp-66) | <1 0 0> | <0 0 1> | 305.9 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 183.5 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 244.7 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 305.9 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 183.5 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 183.5 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 244.7 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 305.9 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 244.7 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 305.9 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 305.9 |
Au (mp-81) | <1 0 0> | <0 0 1> | 305.9 |
Au (mp-81) | <1 1 0> | <0 0 1> | 305.9 |
C (mp-48) | <0 0 1> | <0 0 1> | 305.9 |
C (mp-48) | <1 0 0> | <0 0 1> | 305.9 |
C (mp-48) | <1 1 1> | <0 0 1> | 244.7 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 244.7 |
NaCl (mp-22862) | <1 1 0> | <0 0 1> | 183.5 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 305.9 |
ZrO2 (mp-2858) | <1 1 1> | <0 0 1> | 244.7 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 305.9 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 183.5 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 305.9 |
TiO2 (mp-390) | <1 0 1> | <0 0 1> | 305.9 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 183.5 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 244.7 |
LiAlO2 (mp-3427) | <1 1 0> | <0 0 1> | 183.5 |
CaF2 (mp-2741) | <1 1 0> | <0 0 1> | 305.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SrCa2I6 (mp-780396) | 0.1735 | 0.037 | 3 |
Ba2SrI6 (mp-752671) | 0.2057 | 0.018 | 3 |
Sr2CaI6 (mp-756238) | 0.1915 | 0.022 | 3 |
Fe2CoO6 (mp-772739) | 0.1733 | 0.202 | 3 |
BaSr2I6 (mp-772876) | 0.1564 | 0.017 | 3 |
LiGaPdF6 (mp-9245) | 0.2559 | 0.007 | 4 |
LiMnFeF6 (mp-566418) | 0.2523 | 0.000 | 4 |
LiCdCoF6 (mp-558057) | 0.2922 | 0.044 | 4 |
LiMnFeF6 (mp-648400) | 0.3037 | 0.000 | 4 |
LiTiMnF6 (mp-556715) | 0.2428 | 0.024 | 4 |
Fe2N (mp-684744) | 0.3113 | 0.053 | 2 |
Mn2N (mp-9981) | 0.3145 | 0.000 | 2 |
Co2C (mp-22488) | 0.2575 | 0.110 | 2 |
CaCl2 (mp-571642) | 0.2633 | 0.001 | 2 |
YbBr2 (mp-571232) | 0.2539 | 0.001 | 2 |
Li4ZrNb(TeO6)2 (mp-756177) | 0.6345 | 0.060 | 5 |
SrLaMnRuO6 (mp-39239) | 0.7136 | 0.000 | 5 |
LaMnZnFeO6 (mvc-8951) | 0.6899 | 0.081 | 5 |
LaZnCrWO6 (mvc-9890) | 0.7075 | 0.167 | 5 |
LaZnFeCoO6 (mvc-9020) | 0.7074 | 0.129 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Ca_sv I |
Final Energy/Atom-3.3213 eV |
Corrected Energy-119.5672 eV
-119.5672 eV = -119.5672 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)