Final Magnetic Moment0.348 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.915 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.038 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.92 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBa2(CuO2)3 + Ba2Cu2O5 + Ba2CuO3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 342.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 108.2 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 159.0 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 109.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 162.4 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 228.1 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 238.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 324.7 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 171.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 109.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 285.2 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 1> | 317.9 |
GdScO3 (mp-5690) | <1 1 1> | <1 1 0> | 218.6 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 114.1 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 218.6 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 324.7 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 324.7 |
LaF3 (mp-905) | <1 0 1> | <1 1 0> | 218.6 |
TbScO3 (mp-31119) | <0 0 1> | <0 1 1> | 159.0 |
TbScO3 (mp-31119) | <0 1 1> | <1 1 0> | 109.3 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 228.1 |
TbScO3 (mp-31119) | <1 0 1> | <0 1 0> | 57.0 |
TbScO3 (mp-31119) | <1 1 0> | <0 1 1> | 317.9 |
TbScO3 (mp-31119) | <1 1 1> | <1 1 0> | 218.6 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 171.1 |
Ni (mp-23) | <1 1 1> | <0 1 0> | 171.1 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 270.6 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 162.4 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 1> | 238.5 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 114.1 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 0> | 171.1 |
BaTiO3 (mp-5986) | <1 1 1> | <0 1 0> | 57.0 |
NdGaO3 (mp-3196) | <0 0 1> | <0 1 1> | 159.0 |
NdGaO3 (mp-3196) | <1 0 0> | <0 1 0> | 228.1 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 54.1 |
SiC (mp-11714) | <1 0 0> | <1 1 0> | 218.6 |
SiC (mp-11714) | <1 1 0> | <1 1 0> | 109.3 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 0> | 57.0 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 270.6 |
Ga2O3 (mp-886) | <0 1 0> | <0 0 1> | 270.6 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 54.1 |
Ga2O3 (mp-886) | <1 1 0> | <0 1 0> | 285.2 |
Au (mp-81) | <1 0 0> | <0 1 0> | 171.1 |
Au (mp-81) | <1 1 0> | <0 1 0> | 171.1 |
Au (mp-81) | <1 1 1> | <0 1 1> | 238.5 |
WS2 (mp-224) | <0 0 1> | <0 1 0> | 114.1 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 270.6 |
WS2 (mp-224) | <1 0 1> | <0 0 1> | 270.6 |
C (mp-48) | <0 0 1> | <0 0 1> | 270.6 |
C (mp-48) | <1 0 0> | <0 0 1> | 270.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Cu_pv O |
Final Energy/Atom-5.5954 eV |
Corrected Energy-209.1834 eV
-209.1834 eV = -195.8399 eV (uncorrected energy) - 13.3435 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)