Final Magnetic Moment0.995 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.373 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.043 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH10SeO8 + FeHO2 + Fe2H2Se3O10 + H2O |
Band Gap0.022 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdS (mp-672) | <1 0 0> | <0 0 1> | 316.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 237.1 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 316.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 237.1 |
BN (mp-984) | <1 0 0> | <0 0 1> | 79.0 |
BN (mp-984) | <1 1 0> | <1 0 0> | 133.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 316.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 316.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 237.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 237.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 133.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 316.1 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 237.1 |
C (mp-66) | <1 0 0> | <0 0 1> | 316.1 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 133.7 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 316.1 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 316.1 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 316.1 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 316.1 |
NdGaO3 (mp-3196) | <1 0 0> | <1 0 0> | 133.7 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 0> | 133.7 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 316.1 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 158.1 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 158.1 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 158.1 |
Au (mp-81) | <1 1 1> | <0 0 1> | 237.1 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 133.7 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 316.1 |
SiC (mp-11714) | <1 1 1> | <0 0 1> | 158.1 |
C (mp-48) | <1 0 0> | <1 0 0> | 133.7 |
C (mp-48) | <1 1 0> | <1 0 0> | 133.7 |
Si (mp-149) | <1 0 0> | <0 0 1> | 237.1 |
NaCl (mp-22862) | <1 1 0> | <1 0 0> | 133.7 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 316.1 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 158.1 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 316.1 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 237.1 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 316.1 |
SrTiO3 (mp-4651) | <1 0 0> | <1 0 0> | 133.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ti3H2O7 (mp-626566) | 0.6581 | 0.073 | 3 |
H5IO6 (mp-625890) | 0.7221 | 0.046 | 3 |
TeHO3 (mp-625657) | 0.6963 | 0.027 | 3 |
H5IO6 (mp-625274) | 0.6835 | 0.050 | 3 |
H5IO6 (mp-626014) | 0.6393 | 0.064 | 3 |
Mn3H24(O3F2)4 (mp-743588) | 0.5190 | 0.005 | 4 |
ZnH8(CO2)4 (mp-698274) | 0.4920 | 0.140 | 4 |
VH7(CO2)4 (mp-743895) | 0.3956 | 0.142 | 4 |
ZnH12(SO6)2 (mp-24345) | 0.5134 | 0.024 | 4 |
MgH10(SeO5)2 (mp-24578) | 0.4752 | 0.002 | 4 |
NiSn2H12(OF)6 (mp-735541) | 0.6381 | 0.000 | 5 |
CuSiH12(OF)6 (mp-721943) | 0.5792 | 0.007 | 5 |
CdGaH14O7F5 (mp-561283) | 0.6648 | 0.000 | 5 |
Mn2Cu3H24(OF)12 (mp-541670) | 0.5916 | 0.000 | 5 |
CoSn2H12(OF)6 (mp-601403) | 0.6673 | 0.000 | 5 |
SiH10C2N4(OF3)2 (mp-722686) | 0.7315 | 0.022 | 6 |
ZnHg2H14C4N6O13 (mp-540575) | 0.6995 | 0.312 | 6 |
ReH22C4S4N8Cl8O3 (mp-707926) | 0.7136 | 0.080 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Fe_pv H Se O |
Final Energy/Atom-5.2855 eV |
Corrected Energy-719.4036 eV
-719.4036 eV = -655.4022 eV (uncorrected energy) - 42.1374 eV (MP Anion Correction) - 21.8640 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)