Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.661 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.048 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.79 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiVPO4 + Li3PO4 |
Band Gap3.211 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 294.6 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 293.8 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 153.5 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 172.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 178.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 195.9 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 86.2 |
CeO2 (mp-20194) | <1 1 0> | <1 1 -1> | 207.1 |
GaAs (mp-2534) | <1 0 0> | <1 -1 0> | 245.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 278.3 |
BaF2 (mp-1029) | <1 1 1> | <1 1 -1> | 207.1 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 228.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 178.8 |
GaN (mp-804) | <1 1 1> | <0 1 -1> | 263.6 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 195.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 238.5 |
CeO2 (mp-20194) | <1 1 1> | <1 1 -1> | 51.8 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 228.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 359.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 228.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 -1> | 150.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 -1> | 226.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 332.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 178.8 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 153.5 |
SiO2 (mp-6930) | <0 0 1> | <1 1 -1> | 155.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 280.9 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 276.3 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 290.3 |
KCl (mp-23193) | <1 1 1> | <1 1 -1> | 207.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 -1> | 278.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 276.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 -1> | 310.6 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 -1> | 278.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 228.5 |
InAs (mp-20305) | <1 1 0> | <1 -1 1> | 334.9 |
InAs (mp-20305) | <1 1 1> | <1 1 -1> | 207.1 |
ZnSe (mp-1190) | <1 0 0> | <0 1 -1> | 301.3 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 278.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 214.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 204.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 -1> | 207.1 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 228.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 228.5 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 96.8 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 245.6 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 214.9 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 215.4 |
LiF (mp-1138) | <1 1 1> | <1 1 -1> | 207.1 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 214.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe2SiO4 (mp-698565) | 0.5579 | 0.234 | 3 |
Na4Ti5O12 (mp-760184) | 0.6203 | 0.036 | 3 |
CaMn2O4 (mvc-10181) | 0.5414 | 0.064 | 3 |
Ca(CuO2)2 (mvc-9599) | 0.5924 | 0.261 | 3 |
CaMn2O4 (mvc-10378) | 0.6176 | 0.628 | 3 |
Li7Cr3(WO8)2 (mp-771537) | 0.4992 | 0.057 | 4 |
Li4V5Cu3O16 (mp-777917) | 0.5240 | 0.138 | 4 |
LiMnSiO4 (mp-850949) | 0.4997 | 0.026 | 4 |
LiMn2PO5 (mp-777069) | 0.4854 | 1.412 | 4 |
Li4Mn(PO4)2 (mp-761573) | 0.1622 | 0.055 | 4 |
Li5Mn3Cr(PO4)4 (mp-764909) | 0.4708 | 0.091 | 5 |
Li4Cu3Bi(PO4)4 (mp-765628) | 0.4707 | 0.070 | 5 |
Li4Cu3Sb(PO4)4 (mp-762224) | 0.4813 | 0.070 | 5 |
Li4Ti2V3Ni3O16 (mp-770247) | 0.5224 | 0.064 | 5 |
Li4Cu3Sn(PO4)4 (mp-849752) | 0.4933 | 0.077 | 5 |
Li3MnFeCo(PO4)3 (mp-764912) | 0.6778 | 0.282 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6852 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764708) | 0.6823 | 0.599 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.6852 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6814 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-6.6495 eV |
Corrected Energy-428.1742 eV
-428.1742 eV = -398.9730 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)