Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.540 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.088 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiVO2 + Li2O + LiF |
Band Gap1.652 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 -1> | 201.4 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 303.0 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 -1> | 261.5 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 211.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 78.2 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 260.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 213.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 149.4 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 211.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 156.5 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 242.4 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 273.8 |
BaF2 (mp-1029) | <1 1 0> | <1 1 -1> | 268.5 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 211.2 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 149.4 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 213.3 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 189.6 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 273.8 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 213.3 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 242.4 |
SiO2 (mp-6930) | <0 0 1> | <1 0 -1> | 261.5 |
SiO2 (mp-6930) | <1 1 1> | <1 1 -1> | 268.5 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 211.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 273.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 211.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 273.8 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 112.1 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 278.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 -1> | 224.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 189.6 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 189.6 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 213.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 273.8 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 211.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 336.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 47.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 112.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 312.9 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 303.0 |
CdS (mp-672) | <0 0 1> | <1 0 -1> | 261.5 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 167.3 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 272.5 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 331.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 117.3 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 167.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 260.8 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 118.5 |
Te2W (mp-22693) | <1 1 1> | <1 1 1> | 230.4 |
Te2W (mp-22693) | <1 0 0> | <1 0 -1> | 186.8 |
YVO4 (mp-19133) | <1 0 0> | <1 1 -1> | 134.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.03138 | -0.01024 |
0.29766 | -0.09841 | 0.19391 | -0.11128 | 0.00000 | 0.00000 |
-0.46103 | 0.65978 | 0.14677 | 0.22040 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.88326 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
-0.00000 |
-1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.44 | -0.00 | -0.00 |
-0.00 | 3.01 | -0.03 |
-0.00 | -0.03 | 2.85 |
Dielectric Tensor εij (total) |
||
---|---|---|
9.69 | -0.00 | -0.01 |
-0.00 | 12.08 | -1.13 |
-0.01 | -1.13 | 9.19 |
Polycrystalline dielectric constant
εpoly∞
3.10
|
Polycrystalline dielectric constant
εpoly
10.32
|
Refractive Index n1.76 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5Fe5O12 (mp-771687) | 0.6136 | 0.092 | 3 |
Li2(NiO2)3 (mp-773252) | 0.5828 | 0.241 | 3 |
TlIn5Se7 (mp-574279) | 0.6204 | 0.020 | 3 |
TlIn5S7 (mp-562480) | 0.5811 | 0.000 | 3 |
InBiS3 (mp-1078776) | 0.6050 | 0.003 | 3 |
Li4NbCo5O12 (mp-761963) | 0.5233 | 0.110 | 4 |
Li4V5SnO12 (mp-777449) | 0.5434 | 0.115 | 4 |
Li4Fe5SnO12 (mp-769822) | 0.4892 | 0.197 | 4 |
Li4TiV5O12 (mp-776628) | 0.5535 | 0.109 | 4 |
Li4Co5SbO12 (mp-761626) | 0.5131 | 0.081 | 4 |
In6Se7 (mp-567596) | 0.6192 | 0.042 | 2 |
In6S7 (mp-555853) | 0.5688 | 0.008 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O F |
Final Energy/Atom-5.4971 eV |
Corrected Energy-257.0273 eV
-257.0273 eV = -241.8718 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|