Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.964 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.025 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.89 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
LiVF6
Band Gap
3.155 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P312 [149]
Hall
P 3 2
Point Group
32
Crystal System
trigonal

Electronic Structure

Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ni (mp-23) <1 1 1> <0 0 1> 0.000 21.3
GaN (mp-804) <1 0 0> <1 1 1> 0.003 135.5
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.003 69.0
Al (mp-134) <1 1 1> <0 0 1> 0.004 85.2
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.004 183.9
C (mp-48) <1 1 1> <1 1 1> 0.005 135.5
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.006 191.7
LiAlO2 (mp-3427) <1 1 0> <1 0 1> 0.006 94.0
YAlO3 (mp-3792) <0 0 1> <1 1 1> 0.007 225.8
Fe3O4 (mp-19306) <1 1 0> <1 0 0> 0.008 206.9
Mg (mp-153) <1 1 1> <0 0 1> 0.009 213.1
TePb (mp-19717) <1 1 0> <1 0 0> 0.009 183.9
CeO2 (mp-20194) <1 1 0> <1 0 0> 0.009 252.9
Si (mp-149) <1 1 0> <1 0 0> 0.010 252.9
NdGaO3 (mp-3196) <0 1 1> <1 1 1> 0.010 316.1
DyScO3 (mp-31120) <0 0 1> <1 0 0> 0.011 252.9
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.011 85.2
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.012 277.0
YAlO3 (mp-3792) <1 0 1> <1 0 1> 0.012 344.8
GaN (mp-804) <1 1 1> <0 0 1> 0.012 213.1
C (mp-48) <0 0 1> <0 0 1> 0.013 21.3
BN (mp-984) <0 0 1> <0 0 1> 0.013 149.1
Te2W (mp-22693) <0 0 1> <1 0 1> 0.015 219.4
ZrO2 (mp-2858) <1 1 0> <1 0 1> 0.016 282.1
GdScO3 (mp-5690) <0 1 1> <1 0 0> 0.018 275.9
ZrO2 (mp-2858) <1 0 0> <1 1 1> 0.019 225.8
CdWO4 (mp-19387) <1 1 1> <1 0 0> 0.019 206.9
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.019 85.2
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.019 277.0
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.019 85.2
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.019 277.0
Ni (mp-23) <1 1 0> <1 0 0> 0.022 69.0
Cu (mp-30) <1 0 0> <0 0 1> 0.022 234.4
LiGaO2 (mp-5854) <1 0 1> <1 0 1> 0.023 313.4
CdWO4 (mp-19387) <1 0 0> <1 1 1> 0.023 316.1
YAlO3 (mp-3792) <0 1 0> <1 1 1> 0.025 316.1
SiC (mp-11714) <1 1 1> <1 0 0> 0.025 275.9
Mg (mp-153) <1 0 0> <1 1 1> 0.027 135.5
AlN (mp-661) <1 1 1> <1 0 1> 0.027 313.4
BN (mp-984) <1 0 0> <1 0 0> 0.030 114.9
BaF2 (mp-1029) <1 0 0> <1 0 1> 0.031 156.7
TiO2 (mp-390) <0 0 1> <1 0 1> 0.031 219.4
C (mp-48) <1 1 0> <1 1 1> 0.033 135.5
LiF (mp-1138) <1 1 1> <0 0 1> 0.034 85.2
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.035 255.7
PbSe (mp-2201) <1 0 0> <1 0 1> 0.035 156.7
WS2 (mp-224) <1 1 1> <1 1 1> 0.036 316.1
CdTe (mp-406) <1 1 0> <1 0 0> 0.036 183.9
AlN (mp-661) <1 0 1> <1 1 0> 0.038 159.3
BN (mp-984) <1 1 1> <1 1 1> 0.038 135.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
48 16 12 0 0 0
16 48 12 0 -0 0
12 12 65 0 0 0
0 0 0 13 0 -0
0 -0 0 0 13 0
0 0 0 -0 0 16
Compliance Tensor Sij (10-12Pa-1)
24.1 -7.3 -3.2 0 -1.1 0
-7.3 24.1 -3.2 0 1.1 0
-3.2 -3.2 16.6 0 0 0
0 0 0 79.9 0 2.2
-1.1 1.1 0 0 79.9 0
0 0 0 2.2 0 62.9
Shear Modulus GV
16 GPa
Bulk Modulus KV
27 GPa
Shear Modulus GR
15 GPa
Bulk Modulus KR
27 GPa
Shear Modulus GVRH
16 GPa
Bulk Modulus KVRH
27 GPa
Elastic Anisotropy
0.32
Poisson's Ratio
0.25

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 -0.06123 0.00000 0.06122
0.06122 -0.06122 0.00000 0.00000 0.06123 0.00000
0.00000 0.00000 0.00000 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
0.10604 C/m2
Crystallographic Direction vmax
0.00000
1.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
2.58 -0.00 0.00
-0.00 2.58 0.00
0.00 0.00 2.64
Dielectric Tensor εij (total)
7.15 -0.00 0.00
-0.00 7.15 0.00
0.00 0.00 9.83
Polycrystalline dielectric constant εpoly
(electronic contribution)
2.60
Polycrystalline dielectric constant εpoly
(total)
8.05
Refractive Index n
1.61
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CaPtF6 (mp-8255) 0.2446 0.000 3
CaRhF6 (mp-9928) 0.2588 0.000 3
MgNiF6 (mvc-15858) 0.2675 0.000 3
NaBiF6 (mp-27420) 0.2496 0.000 3
TiCdF6 (mp-623024) 0.2562 0.000 3
CsAlCuF6 (mp-510370) 0.6920 0.000 4
Cs2LiAl3F12 (mp-13634) 0.4740 0.000 4
TeO3 (mvc-2186) 0.4550 0.033 2
MnF3 (mp-766789) 0.3419 0.031 2
NiF3 (mp-614777) 0.2807 0.000 2
NiF3 (mp-561428) 0.4537 0.000 2
TeO3 (mp-2552) 0.4652 0.020 2
CsMnMo(OF)3 (mp-699398) 0.7408 0.070 5
TiNbTl(O2F)2 (mp-677378) 0.7334 0.045 5
TiTlWO5F (mp-690560) 0.6276 0.000 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
V: 3.25 eV
Pseudopotentials
VASP PAW: Li_sv V_pv F
Final Energy/Atom
-5.1930 eV
Corrected Energy
-43.2259 eV
-43.2259 eV = -41.5439 eV (uncorrected energy) - 1.6820 eV (MP Advanced Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)