Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.762 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.085 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV2O3 + Li2Si2O5 |
Band Gap2.208 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 312.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 134.0 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 55.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 223.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 89.4 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 204.6 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 165.8 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 55.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 223.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 134.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 134.0 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 145.0 |
CdS (mp-672) | <1 0 1> | <1 1 -1> | 263.3 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 268.1 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 72.5 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 217.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 165.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 134.0 |
YVO4 (mp-19133) | <1 1 1> | <1 0 -1> | 165.8 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 139.4 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 89.4 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 46.5 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 221.1 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 163.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 92.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 217.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 217.5 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 272.8 |
BN (mp-984) | <0 0 1> | <1 0 -1> | 276.4 |
BN (mp-984) | <1 1 1> | <0 1 0> | 68.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 298.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 134.0 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 -1> | 276.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 217.5 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 278.8 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 268.1 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 325.3 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 139.4 |
MoS2 (mp-1434) | <1 1 0> | <1 0 0> | 232.3 |
MoS2 (mp-1434) | <1 1 1> | <1 0 0> | 232.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 325.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 268.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 134.0 |
Al (mp-134) | <1 0 0> | <0 0 1> | 134.0 |
Al (mp-134) | <1 1 0> | <1 1 1> | 298.6 |
BN (mp-984) | <1 0 1> | <1 0 -1> | 165.8 |
BN (mp-984) | <1 1 0> | <1 0 0> | 325.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 -1> | 55.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 325.3 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 1> | 290.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
B2(CN2)3 (mp-989468) | 0.5408 | 0.437 | 3 |
Be(GaO2)2 (mp-676950) | 0.4046 | 0.116 | 3 |
Li2CrO4 (mp-769767) | 0.5531 | 0.020 | 3 |
Zn2SiO4 (mp-1020721) | 0.4923 | 0.111 | 3 |
Zn2SiO4 (mp-1020636) | 0.5399 | 0.052 | 3 |
LiCuPO4 (mp-758520) | 0.2685 | 0.067 | 4 |
LiCoSiO4 (mp-763592) | 0.1383 | 0.231 | 4 |
LiFeSiO4 (mp-762656) | 0.2789 | 0.070 | 4 |
LiFeSiO4 (mp-762645) | 0.1439 | 0.430 | 4 |
LiAlSiO4 (mp-556544) | 0.2790 | 0.022 | 4 |
Ge3N4 (mp-672289) | 0.7419 | 0.000 | 2 |
Cr3N4 (mp-1014369) | 0.7117 | 0.164 | 2 |
Si3N4 (mp-2245) | 0.7386 | 0.000 | 2 |
CN2 (mp-1077595) | 0.7015 | 0.691 | 2 |
Ti3N4 (mp-1080190) | 0.7006 | 0.119 | 2 |
Be3Fe4Si3SO12 (mp-627398) | 0.6852 | 0.203 | 5 |
YAl6Si18(N15O)2 (mp-677127) | 0.6732 | 0.092 | 5 |
Li4Ga3Si3IO12 (mp-557112) | 0.6865 | 0.000 | 5 |
LaAl2Si5N9O (mp-677482) | 0.6730 | 0.151 | 5 |
YAl6Si30(N15O)3 (mp-677140) | 0.6886 | 0.084 | 5 |
Na2Li2Al3Si3ClO12 (mp-43030) | 0.6124 | 0.003 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Si O |
Final Energy/Atom-7.2932 eV |
Corrected Energy-222.1746 eV
-222.1746 eV = -204.2099 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)