Final Magnetic Moment21.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.156 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.055 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.24 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMn2O3 + Mn3O4 + LiF |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [160] |
HallR 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 230.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 295.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 164.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 230.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 272.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 295.9 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 263.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 295.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 230.1 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 98.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 230.1 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 289.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 230.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 164.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 32.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 164.4 |
Te2Mo (mp-602) | <1 1 1> | <1 0 1> | 96.5 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 230.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 193.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 131.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 295.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 230.1 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 193.1 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 263.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 98.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 295.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 65.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 230.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 164.4 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 230.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 263.0 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 32.9 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 98.6 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 295.9 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 131.5 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 131.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 361.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 230.1 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 295.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 131.5 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 361.6 |
SiC (mp-7631) | <1 0 0> | <1 0 1> | 96.5 |
SiC (mp-7631) | <1 1 0> | <1 1 1> | 160.6 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 164.4 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 32.9 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 263.0 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 157.2 |
C (mp-66) | <1 0 0> | <0 0 1> | 263.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 263.0 |
C (mp-66) | <1 1 1> | <0 0 1> | 295.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cd(GaO2)2 (mp-531238) | 0.3681 | 0.023 | 3 |
Mg(CuO2)2 (mvc-9578) | 0.3488 | 0.065 | 3 |
Cd(GaO2)2 (mp-531175) | 0.3604 | 0.035 | 3 |
CaV2O4 (mvc-10172) | 0.3343 | 0.042 | 3 |
Ca(FeO2)2 (mvc-10242) | 0.3469 | 0.053 | 3 |
LiMn5O3F5 (mp-763431) | 0.3378 | 0.086 | 4 |
LiV5O7F (mp-765835) | 0.3651 | 0.047 | 4 |
Li2Mn3SnO8 (mp-773330) | 0.3044 | 0.098 | 4 |
LiMn2O3F (mp-765331) | 0.2595 | 0.340 | 4 |
LiMn3(FeO4)2 (mp-773282) | 0.3374 | 0.104 | 4 |
FeP4 (mp-27164) | 0.5362 | 0.001 | 2 |
P4Ru (mp-27173) | 0.5284 | 0.000 | 2 |
Ni3S4 (mp-1050) | 0.5418 | 0.000 | 2 |
Mn3N4 (mp-1080204) | 0.5176 | 0.172 | 2 |
Cr3N4 (mp-1014358) | 0.4603 | 0.227 | 2 |
Li4Mn3Co2Ni3O16 (mp-868013) | 0.4103 | 0.078 | 5 |
Li4Ti3Co3(SbO8)2 (mp-773988) | 0.4105 | 0.041 | 5 |
Li4Ti3Mn3V2O16 (mp-770420) | 0.4101 | 0.087 | 5 |
Li4V3Ni2Sn3O16 (mp-777392) | 0.4015 | 0.081 | 5 |
Li4V3Cr2Fe3O16 (mp-778220) | 0.4101 | 0.882 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6117 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6100 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.6147 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6112 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6125 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv O F |
Final Energy/Atom-7.1885 eV |
Corrected Energy-113.9588 eV
-113.9588 eV = -100.6385 eV (uncorrected energy) - 8.4043 eV (MP Advanced Correction) - 4.9160 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)