Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.636 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.039 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLa2Ti2O7 + Li4Ti5O12 + TiO2 |
Band Gap2.117 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 52.7 |
AlN (mp-661) | <1 0 1> | <0 1 -1> | 303.4 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 172.9 |
GaN (mp-804) | <0 0 1> | <0 1 -1> | 303.4 |
GaN (mp-804) | <1 1 1> | <0 1 -1> | 60.7 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 172.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 122.7 |
InAs (mp-20305) | <1 0 0> | <0 1 -1> | 303.4 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 211.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 158.2 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 1> | 259.3 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 259.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 105.4 |
LiF (mp-1138) | <1 0 0> | <0 1 -1> | 303.4 |
AlN (mp-661) | <0 0 1> | <0 1 -1> | 303.4 |
AlN (mp-661) | <1 1 0> | <0 1 -1> | 242.7 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 203.1 |
CeO2 (mp-20194) | <1 0 0> | <0 1 -1> | 60.7 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 86.4 |
CeO2 (mp-20194) | <1 1 1> | <0 1 -1> | 303.4 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 203.1 |
BaF2 (mp-1029) | <1 0 0> | <0 1 -1> | 303.4 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 101.5 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 86.4 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 259.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 316.3 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 210.9 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 263.6 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 316.3 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 158.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 -1> | 242.7 |
SiO2 (mp-6930) | <1 1 0> | <0 1 -1> | 242.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 158.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 86.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 52.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 263.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 210.9 |
Te2Mo (mp-602) | <0 0 1> | <0 1 -1> | 303.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 158.7 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 259.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 -1> | 303.4 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 316.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 105.4 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 52.7 |
MoS2 (mp-1434) | <1 0 0> | <1 1 0> | 203.1 |
Al (mp-134) | <1 0 0> | <0 1 1> | 259.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 -1> | 303.4 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 105.4 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 -1> | 182.1 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 263.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La11Mn12O36 (mp-768328) | 0.6674 | 0.207 | 3 |
La15Mn16O48 (mp-773935) | 0.6755 | 0.191 | 3 |
La17Mn17O54 (mp-705870) | 0.6844 | 0.228 | 3 |
La5Mn5O18 (mp-690531) | 0.6785 | 0.254 | 3 |
La7Mn8O24 (mp-698566) | 0.6824 | 0.208 | 3 |
LiLa3Ti4O12 (mp-752433) | 0.6844 | 0.029 | 4 |
LiCa2Ta3O10 (mp-774479) | 0.7046 | 0.068 | 4 |
Sr2LiNb3O10 (mp-756854) | 0.5618 | 0.043 | 4 |
La3Ti3CrO12 (mp-769844) | 0.7146 | 0.045 | 4 |
La2Ti2CrO9 (mp-767602) | 0.6866 | 0.053 | 4 |
BaLaMnInO6 (mp-697820) | 0.6196 | 0.119 | 5 |
CaLa2Ti2Cr2O12 (mvc-13117) | 0.6286 | 0.098 | 5 |
Na2LiLa3Ti6O18 (mp-676447) | 0.5968 | 0.025 | 5 |
CaLa2Ti2Mn2O12 (mvc-14929) | 0.6238 | 0.132 | 5 |
Na11La7Th2Ti20O60 (mp-686371) | 0.6299 | 0.017 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv La Ti_pv O |
Final Energy/Atom-8.6799 eV |
Corrected Energy-346.6897 eV
-346.6897 eV = -329.8347 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)