Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.492 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.529 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 0> | <0 0 1> | 273.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 -1> | 173.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 273.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 273.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 273.5 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 173.3 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 173.3 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 182.4 |
BN (mp-984) | <1 1 1> | <0 0 1> | 273.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 273.5 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 -1> | 173.3 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 273.5 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 155.3 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 155.3 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 155.3 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 273.5 |
Au (mp-81) | <1 0 0> | <1 0 -1> | 173.3 |
C (mp-48) | <0 0 1> | <0 0 1> | 273.5 |
C (mp-48) | <1 1 1> | <0 0 1> | 273.5 |
C (mp-48) | <1 1 0> | <0 0 1> | 273.5 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 273.5 |
ZnO (mp-2133) | <1 0 0> | <1 0 -1> | 173.3 |
GaTe (mp-542812) | <0 0 1> | <1 0 0> | 155.3 |
GaTe (mp-542812) | <1 0 -1> | <1 0 0> | 155.3 |
GaTe (mp-542812) | <1 0 0> | <0 0 1> | 91.2 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 273.5 |
LiAlO2 (mp-3427) | <1 0 0> | <0 0 1> | 273.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr5Mo2N7 (mp-31231) | 0.6129 | 0.000 | 3 |
Tb3S3N (mp-18164) | 0.7208 | 0.000 | 3 |
Sm3S3N (mp-4038) | 0.6863 | 0.001 | 3 |
Nd3S3N (mp-554001) | 0.6954 | 0.000 | 3 |
Gd3S3N (mp-647096) | 0.7060 | 0.000 | 3 |
Cu2Bi4Pb2S9 (mp-652196) | 0.7366 | 0.007 | 4 |
Rb2NaMnO4 (mp-18873) | 0.6488 | 0.000 | 4 |
Cs2NaVO4 (mp-19447) | 0.7263 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Li_sv V_pv S |
Final Energy/Atom-4.8802 eV |
Corrected Energy-164.2145 eV
Uncorrected energy = -156.1665 eV
Composition-based energy adjustment (-0.503 eV/atom x 16.0 atoms) = -8.0480 eV
Corrected energy = -164.2145 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)