Final Magnetic Moment10.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.379 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.027 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.63 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3Cr2(PO4)3 + LiNiPO4 + Ni |
Band Gap1.539 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm [6] |
HallP 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 224.2 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 234.1 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 337.3 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 203.8 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 234.1 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 184.1 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 135.9 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 312.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 143.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 271.8 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 280.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 143.2 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 280.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 289.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 85.9 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 337.3 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 184.1 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 184.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 143.2 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 122.7 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 61.4 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 200.5 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 192.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 114.6 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 280.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 114.6 |
BN (mp-984) | <1 0 0> | <1 1 0> | 78.0 |
BN (mp-984) | <1 0 1> | <0 0 1> | 315.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 229.1 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 337.3 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 271.8 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 336.3 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 200.5 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 184.1 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 144.6 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 0> | 306.8 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 257.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 280.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 114.6 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 257.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 1> | 280.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 245.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 286.4 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 144.6 |
CdS (mp-672) | <1 1 0> | <1 1 1> | 249.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 245.5 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 234.1 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 306.8 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 192.7 |
TePb (mp-19717) | <1 0 0> | <0 1 1> | 224.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn2SiO4 (mp-1020609) | 0.2596 | 0.083 | 3 |
V2SiO4 (mp-772381) | 0.2445 | 0.000 | 3 |
Mn2SiO4 (mp-18928) | 0.1924 | 0.000 | 3 |
Fe2SiO4 (mp-510587) | 0.2258 | 0.000 | 3 |
Ca2GeO4 (mp-560647) | 0.2408 | 0.000 | 3 |
Li5Mn3(PO4)4 (mp-771623) | 0.1565 | 0.012 | 4 |
Li3Fe(PO4)2 (mp-773399) | 0.1425 | 0.012 | 4 |
LiNiPO4 (mp-763217) | 0.1328 | 0.050 | 4 |
LiCoPO4 (mp-18915) | 0.1472 | 0.057 | 4 |
LiCuPO4 (mp-25449) | 0.1777 | 0.035 | 4 |
Fe3O4 (mp-715491) | 0.6585 | 0.017 | 2 |
Mn3N4 (mp-1080204) | 0.6388 | 0.172 | 2 |
Cr3N4 (mp-1014358) | 0.5563 | 0.227 | 2 |
Fe3O4 (mp-650112) | 0.6359 | 0.060 | 2 |
Fe3O4 (mp-716052) | 0.6581 | 0.781 | 2 |
Li4CuNi3(PO4)4 (mp-767664) | 0.0746 | 0.014 | 5 |
Li4CrCo3(PO4)4 (mp-762038) | 0.0570 | 0.035 | 5 |
Li2CrNi(PO4)2 (mp-761997) | 0.0852 | 0.047 | 5 |
Li2CoCu(PO4)2 (mp-769707) | 0.1158 | 0.041 | 5 |
Li2CrCo(PO4)2 (mp-761707) | 0.0972 | 0.035 | 5 |
Li3MnFeCo(PO4)3 (mp-764912) | 0.1227 | 0.282 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.1282 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.1287 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.1296 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.1300 | 0.057 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv Ni_pv P O |
Final Energy/Atom-6.5111 eV |
Corrected Energy-202.0518 eV
-202.0518 eV = -182.3102 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 8.5050 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)