Final Magnetic Moment15.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.758 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.071 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.69 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnO + MnF2 + LiF |
Band Gap1.894 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 1> | <0 1 0> | 120.2 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 231.1 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 231.1 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 173.7 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 320.5 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 216.9 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 115.5 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 200.3 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 200.3 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 72.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 320.5 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 216.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 80.1 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 231.1 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 320.5 |
Te2W (mp-22693) | <1 0 0> | <0 1 1> | 288.9 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 72.3 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 289.2 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 289.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 200.3 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 320.5 |
GaSe (mp-1943) | <1 0 1> | <0 1 1> | 288.9 |
Al (mp-134) | <1 0 0> | <1 0 0> | 80.8 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 1> | 231.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 173.3 |
CdTe (mp-406) | <1 0 0> | <0 1 1> | 173.3 |
CdTe (mp-406) | <1 1 1> | <1 1 1> | 72.3 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 121.2 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 173.7 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 240.3 |
SiC (mp-7631) | <1 0 0> | <0 1 1> | 288.9 |
SiC (mp-7631) | <1 0 1> | <0 1 1> | 288.9 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 231.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 57.9 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 72.3 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 120.2 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 280.4 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 72.3 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 240.3 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 288.9 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 57.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 160.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 173.7 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 231.1 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 216.9 |
TiO2 (mp-2657) | <0 0 1> | <0 1 1> | 173.3 |
TiO2 (mp-2657) | <1 0 0> | <1 1 1> | 289.2 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 200.3 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 200.3 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 115.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sn2N2O (mp-766117) | 0.2884 | 0.068 | 3 |
Sn2N2O (mp-762250) | 0.3071 | 0.061 | 3 |
Sn2N2O (mp-773831) | 0.3011 | 0.059 | 3 |
Sn2N2O (mp-758863) | 0.2894 | 0.064 | 3 |
Sn2N2O (mp-777302) | 0.2898 | 0.058 | 3 |
LiMn7(O3F)3 (mp-765039) | 0.3758 | 0.089 | 4 |
Li2Co4OF8 (mp-765686) | 0.3983 | 0.077 | 4 |
Li2Fe4OF8 (mp-849951) | 0.3935 | 0.057 | 4 |
LiCo3OF5 (mp-850139) | 0.2142 | 0.091 | 4 |
LiFe3OF5 (mp-764579) | 0.1614 | 0.086 | 4 |
Fe2O3 (mp-777192) | 0.3656 | 0.123 | 2 |
Fe2O3 (mp-715572) | 0.4308 | 0.077 | 2 |
FeP4 (mp-27164) | 0.4894 | 0.001 | 2 |
Rh2O3 (mp-613620) | 0.4651 | 0.027 | 2 |
V2O3 (mp-849288) | 0.4830 | 0.031 | 2 |
Li4V2Cr3Sb3O16 (mp-775451) | 0.4509 | 0.098 | 5 |
Li4Fe3Co2Sn3O16 (mp-775387) | 0.4816 | 0.111 | 5 |
Li4V2Cr3Fe3O16 (mp-770523) | 0.4690 | 0.892 | 5 |
Li4Fe3Co2Cu3O16 (mp-763163) | 0.4540 | 0.089 | 5 |
Li4Mn3V3(WO8)2 (mp-763077) | 0.4651 | 0.034 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv O F |
Final Energy/Atom-6.3286 eV |
Corrected Energy-138.0613 eV
-138.0613 eV = -126.5717 eV (uncorrected energy) - 10.0851 eV (MP Advanced Correction) - 1.4046 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)