Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.664 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.029 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2CO3 + AlPO4 |
Band Gap5.714 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <0 0 1> | <1 1 0> | 133.3 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 186.4 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 251.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 279.7 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 155.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 217.5 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 217.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 217.5 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 293.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 224.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 310.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 167.7 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 117.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 217.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 341.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 248.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 207.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 310.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 310.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 248.6 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 224.9 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 251.5 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 248.6 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 209.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 310.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 155.4 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 93.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 310.7 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 176.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 62.1 |
YVO4 (mp-19133) | <1 1 1> | <0 0 1> | 248.6 |
TePb (mp-19717) | <1 0 0> | <1 0 -1> | 176.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 155.4 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 93.2 |
Te2Mo (mp-602) | <1 1 1> | <1 0 1> | 186.4 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 176.0 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 209.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 155.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 155.4 |
BN (mp-984) | <1 0 1> | <1 1 0> | 200.0 |
BN (mp-984) | <1 1 0> | <1 0 -1> | 234.6 |
BN (mp-984) | <1 1 1> | <0 1 0> | 167.7 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 217.5 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 313.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 31.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 217.5 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 133.3 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 224.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 310.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 341.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CuSeO4 (mp-554040) | 0.7460 | 0.000 | 3 |
Li3V(BO2)5 (mp-770344) | 0.5894 | 0.111 | 4 |
Li9Cr4(BO3)8 (mp-763230) | 0.6377 | 0.086 | 4 |
Na3Ca(BO2)5 (mp-614628) | 0.6652 | 0.002 | 4 |
Li9Cr4(BO3)8 (mp-765270) | 0.6484 | 0.075 | 4 |
Li3Ni(BO2)5 (mp-771081) | 0.6375 | 0.092 | 4 |
Li2NiCSO7 (mp-771489) | 0.3625 | 0.061 | 5 |
Li2FeBPO7 (mp-778767) | 0.1724 | 0.259 | 5 |
Na2FeBAsO7 (mp-771805) | 0.3745 | 0.251 | 5 |
Li2CoPCO7 (mp-25482) | 0.3117 | 0.050 | 5 |
Li2FePCO7 (mp-25528) | 0.3450 | 0.015 | 5 |
Li12Mn3VP4(CO7)4 (mp-767666) | 0.6550 | 0.054 | 6 |
Li6MnCoP2(CO7)2 (mp-767318) | 0.6579 | 0.053 | 6 |
Li6MnNiP2(CO7)2 (mp-767293) | 0.6529 | 0.046 | 6 |
Li6VCrP2(CO7)2 (mp-767288) | 0.6551 | 0.080 | 6 |
NaLiMnPCO7 (mp-763833) | 0.5390 | 0.062 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Al P C O |
Final Energy/Atom-6.9912 eV |
Corrected Energy-177.6207 eV
-177.6207 eV = -167.7887 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)