Final Magnetic Moment7.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.189 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.088 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3CrO4 + Li3SbO4 + LiCrO2 |
Band Gap0.625 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2 [3] |
HallP 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 198.4 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 258.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 126.6 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 248.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 214.3 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 126.6 |
GaAs (mp-2534) | <1 1 0> | <1 1 1> | 330.7 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 199.2 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 202.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 303.9 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 278.6 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 126.6 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 227.9 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 250.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 42.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 199.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 214.3 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 301.9 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 199.2 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 183.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 126.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 171.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 264.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 126.6 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 199.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 214.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 128.6 |
ZnSe (mp-1190) | <1 1 0> | <1 1 1> | 330.7 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 126.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 126.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 330.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 199.2 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 244.4 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 61.1 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 278.6 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 129.4 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 264.6 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 330.7 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 126.6 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 199.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 257.2 |
Te2W (mp-22693) | <0 1 1> | <0 1 1> | 298.7 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 177.3 |
Te2W (mp-22693) | <1 1 1> | <0 1 0> | 227.9 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 50.6 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 183.3 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 202.6 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 329.2 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 227.9 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 177.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5CuF6 (mp-760782) | 0.3888 | 0.106 | 3 |
Li2CrO3 (mp-764409) | 0.1861 | 0.102 | 3 |
LiMoO2 (mp-690493) | 0.4779 | 0.035 | 3 |
LiMoS2 (mp-30248) | 0.4252 | 0.023 | 3 |
Li2FeO3 (mp-764638) | 0.2626 | 0.067 | 3 |
Li8Cr(FeO4)3 (mp-767681) | 0.2227 | 1.033 | 4 |
Li8TiMn3O12 (mp-767679) | 0.1976 | 0.088 | 4 |
Li8Mn(FeO4)3 (mp-766973) | 0.2216 | 0.073 | 4 |
Li8MnCr3O12 (mp-766919) | 0.1497 | 0.112 | 4 |
Li8Mn3CrO12 (mp-765119) | 0.2051 | 0.107 | 4 |
FeO (mp-849689) | 0.5431 | 0.104 | 2 |
MoN (mp-2811) | 0.5797 | 0.000 | 2 |
FeO (mp-756436) | 0.5244 | 0.116 | 2 |
KAs (mp-1078831) | 0.5999 | 0.848 | 2 |
KI (mp-1078836) | 0.5969 | 0.019 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.6427 | 0.005 | 5 |
Na (mp-999501) | 0.7385 | 0.124 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv Sb O |
Final Energy/Atom-6.0753 eV |
Corrected Energy-160.2743 eV
-160.2743 eV = -145.8078 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 6.0390 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)