Final Magnetic Moment0.261 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.310 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.044 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.40 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiV2O5 + V2O5 + VO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 282.9 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 237.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 188.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 225.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 112.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 112.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 237.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 338.4 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 112.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 225.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 112.8 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 237.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 263.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 112.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 300.8 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 338.4 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 158.5 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 112.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 338.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 241.8 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 112.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 75.2 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 282.9 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 150.4 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 158.5 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 263.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 188.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 263.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 158.5 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 317.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 75.2 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 263.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 263.2 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 263.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 241.8 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 112.8 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 112.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 263.2 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 75.2 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 263.2 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 338.4 |
BN (mp-984) | <1 0 1> | <0 0 1> | 263.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 188.0 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 188.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 188.0 |
MoS2 (mp-1434) | <0 0 1> | <1 0 1> | 282.9 |
MoS2 (mp-1434) | <1 1 0> | <1 0 0> | 237.8 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 300.8 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 237.8 |
C (mp-66) | <1 1 0> | <0 0 1> | 37.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiV18O44 (mp-775458) | 0.3323 | 0.033 | 3 |
LiV9O22 (mp-773986) | 0.3332 | 0.045 | 3 |
NaV24O58 (mp-765714) | 0.3230 | 0.031 | 3 |
LiV6O15 (mp-776036) | 0.2802 | 0.021 | 3 |
LiV24O58 (mp-765490) | 0.3099 | 0.030 | 3 |
BaNb3NO7 (mp-755621) | 0.7158 | 0.076 | 4 |
V9O22 (mp-850238) | 0.2791 | 0.035 | 2 |
V4O9 (mp-715596) | 0.5446 | 0.025 | 2 |
V12O29 (mp-774272) | 0.3002 | 0.033 | 2 |
V2O5 (mp-25646) | 0.4271 | 0.030 | 2 |
V4O9 (mp-504533) | 0.5702 | 0.025 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O |
Final Energy/Atom-7.3695 eV |
Corrected Energy-532.4780 eV
Uncorrected energy = -471.6500 eV
Composition-based energy adjustment (-0.687 eV/atom x 44.0 atoms) = -30.2280 eV
Composition-based energy adjustment (-1.700 eV/atom x 18.0 atoms) = -30.6000 eV
Corrected energy = -532.4780 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)