Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.601 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.006 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVP2O7 + LiFeP2O7 |
Band Gap1.605 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 276.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 153.3 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 118.5 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 276.6 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 197.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 259.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 227.1 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 197.5 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 204.4 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 199.1 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 79.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 259.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 227.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 292.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 -1 1> | 255.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 -1 1> | 85.1 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 197.5 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 79.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 283.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 -1 0> | 157.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 197.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 197.5 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 197.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 1> | 331.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 170.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 227.1 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 255.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 292.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 292.0 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 261.0 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 227.1 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 132.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 227.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 197.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 292.0 |
InAs (mp-20305) | <1 1 0> | <1 1 1> | 265.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 227.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 292.0 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 227.1 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 326.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 227.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 194.6 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 261.0 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 227.1 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 290.3 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 259.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 170.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 97.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 356.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 227.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V5(P3O11)2 (mp-767351) | 0.3326 | 0.023 | 3 |
Co5(P3O11)2 (mp-31617) | 0.3646 | 0.034 | 3 |
Ni5(P3O11)2 (mp-32359) | 0.2987 | 0.082 | 3 |
Mn5(P3O11)2 (mp-705036) | 0.4182 | 0.028 | 3 |
Fe5(P3O11)2 (mp-705342) | 0.3422 | 0.038 | 3 |
LiVP2O7 (mp-18911) | 0.2914 | 0.033 | 4 |
LiFeP2O7 (mp-19294) | 0.2923 | 0.000 | 4 |
LiScP2O7 (mp-10517) | 0.3148 | 0.000 | 4 |
LiTiP2O7 (mp-26629) | 0.2886 | 0.055 | 4 |
LiCoP2O7 (mp-31535) | 0.2791 | 0.057 | 4 |
LiVCr(P2O7)2 (mp-767608) | 0.0603 | 0.007 | 5 |
LiVCr(P2O7)2 (mp-765174) | 0.1273 | 0.009 | 5 |
LiVFe(P2O7)2 (mp-765127) | 0.1265 | 0.008 | 5 |
LiVCr(P2O7)2 (mp-765163) | 0.1215 | 0.009 | 5 |
LiVFe(P2O7)2 (mp-765179) | 0.1268 | 0.008 | 5 |
NaLi5Ti3Cr3(PO4)9 (mp-744549) | 0.7421 | 0.059 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.4597 | 0.255 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.4911 | 0.330 | 6 |
CsAlBP2HO9 (mp-542129) | 0.7284 | 0.000 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5852 | 0.002 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Fe_pv P O |
Final Energy/Atom-7.1787 eV |
Corrected Energy-329.9995 eV
-329.9995 eV = -301.5054 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 8.8300 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)