Final Magnetic Moment3.014 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.381 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.056 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.77 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiV(CO3)2 + V2CoO4 + LiCoPO4 + CoCO3 + Li3PO4 + C |
Band Gap0.872 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm [6] |
HallP 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 196.4 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 123.7 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 168.1 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 236.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 163.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 360.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 276.9 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 123.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 294.6 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 309.2 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 -1> | 309.2 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 -1> | 123.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 229.2 |
AlN (mp-661) | <1 0 1> | <1 1 -1> | 299.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 163.7 |
AlN (mp-661) | <1 1 1> | <1 1 -1> | 224.3 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 213.1 |
CeO2 (mp-20194) | <1 1 1> | <1 0 -1> | 247.3 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 319.7 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 66.8 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 208.6 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 200.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 327.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 210.2 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 319.7 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 168.1 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 276.9 |
MoS2 (mp-1434) | <1 0 1> | <1 0 0> | 276.9 |
Al (mp-134) | <1 1 0> | <0 1 0> | 210.2 |
Al (mp-134) | <1 1 1> | <0 0 1> | 196.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 210.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 196.4 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 210.2 |
CdS (mp-672) | <1 0 0> | <1 1 -1> | 224.3 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 236.6 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 252.2 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 261.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 163.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 32.7 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 221.6 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 110.8 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 276.9 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 98.2 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 163.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 261.9 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 168.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 196.4 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 130.9 |
CdTe (mp-406) | <1 1 0> | <1 0 -1> | 61.8 |
CdTe (mp-406) | <1 1 1> | <1 0 -1> | 309.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3Fe3(BO3)4 (mp-767662) | 0.6630 | 0.091 | 4 |
Li3Si2Bi3O10 (mp-757200) | 0.7293 | 0.053 | 4 |
Li9V12Te7O48 (mp-849282) | 0.7057 | 0.057 | 4 |
Li3CoPCO7 (mp-767912) | 0.2104 | 0.173 | 5 |
Li3VPCO7 (mp-767894) | 0.1234 | 0.088 | 5 |
Li3NiPCO7 (mp-767883) | 0.1784 | 0.096 | 5 |
Li3VPCO7 (mp-767879) | 0.2119 | 0.172 | 5 |
Li3NiPCO7 (mp-767869) | 0.2304 | 0.235 | 5 |
Li12V3FeP4(CO7)4 (mp-767693) | 0.0449 | 0.061 | 6 |
Li12CoNi3P4(CO7)4 (mp-767857) | 0.0754 | 0.036 | 6 |
Li12V3CoP4(CO7)4 (mp-767842) | 0.0799 | 0.095 | 6 |
Li12VFe3P4(CO7)4 (mp-767730) | 0.0874 | 0.047 | 6 |
Li6FeCoP2(CO7)2 (mp-767298) | 0.0891 | 0.132 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Co P C O |
Final Energy/Atom-6.7198 eV |
Corrected Energy-376.2039 eV
-376.2039 eV = -349.4277 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 7.1120 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)