Final Magnetic Moment16.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.670 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.069 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.47 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi9Mn20O40 + Mn(Cu3O4)2 + MnO2 |
Band Gap0.298 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 140.1 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 250.8 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 309.3 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 154.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 206.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 186.8 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 196.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 186.8 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 139.1 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 206.2 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 206.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 167.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 233.5 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 271.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 233.5 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 167.2 |
BaF2 (mp-1029) | <1 1 1> | <1 0 -1> | 271.5 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 250.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 186.8 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 206.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 233.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 46.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 93.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 257.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 326.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 309.3 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 208.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 309.3 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 226.3 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 208.7 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 201.5 |
BN (mp-984) | <0 0 1> | <0 1 1> | 208.7 |
BN (mp-984) | <1 1 0> | <1 0 -1> | 271.5 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 257.7 |
YVO4 (mp-19133) | <1 1 0> | <1 0 -1> | 271.5 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 257.7 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 208.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 271.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 140.1 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 -1> | 271.5 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 257.7 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 140.1 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 309.3 |
BN (mp-984) | <1 1 1> | <1 0 -1> | 271.5 |
TeO2 (mp-2125) | <0 0 1> | <1 1 1> | 226.3 |
TeO2 (mp-2125) | <1 1 1> | <0 1 1> | 208.7 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 140.1 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 233.5 |
MoS2 (mp-1434) | <1 1 1> | <0 0 1> | 233.5 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 206.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(CoO2)3 (mp-997539) | 0.3780 | 0.105 | 3 |
LiMn3O6 (mp-762404) | 0.3186 | 0.174 | 3 |
Li3Fe5O12 (mp-762739) | 0.3423 | 0.145 | 3 |
LiMn7O12 (mp-763608) | 0.2829 | 0.068 | 3 |
LiTi3O6 (mp-752891) | 0.3672 | 0.039 | 3 |
Li2Mn3(FeO4)3 (mp-767665) | 0.3837 | 0.095 | 4 |
Li2Ti3V3O12 (mp-763640) | 0.3902 | 0.091 | 4 |
Li2Fe4OF8 (mp-849951) | 0.3787 | 0.057 | 4 |
Li3Ni5OF11 (mp-765843) | 0.3732 | 0.113 | 4 |
LiV2CrO6 (mp-849360) | 0.3520 | 0.107 | 4 |
Fe2O3 (mp-777192) | 0.5228 | 0.732 | 2 |
Al2O3 (mp-755175) | 0.5109 | 0.072 | 2 |
Al2O3 (mp-754624) | 0.4866 | 0.065 | 2 |
Sc2O3 (mp-754455) | 0.4905 | 0.086 | 2 |
Mn2O3 (mp-565203) | 0.5420 | 0.000 | 2 |
Li4CrBi(TeO6)2 (mp-775998) | 0.6331 | 0.076 | 5 |
Li4Fe2TeWO12 (mp-768021) | 0.5809 | 0.083 | 5 |
Li4VFe(TeO6)2 (mp-761819) | 0.6259 | 0.060 | 5 |
Li4MnV2WO12 (mp-773239) | 0.5884 | 0.089 | 5 |
Li4V2CrTeO12 (mp-775632) | 0.5932 | 0.104 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Cu_pv O |
Final Energy/Atom-6.5930 eV |
Corrected Energy-148.6908 eV
-148.6908 eV = -131.8591 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 8.4043 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)