material

VOF

ID:

mp-767367

DOI:

10.17188/1297570


Material Details

Final Magnetic Moment
8.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-2.810 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.039 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.50 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
VOF
Band Gap
1.999 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P212121 [19]
Hall
P 2ac 2ab
Point Group
222
Crystal System
orthorhombic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LiF (mp-1138) <1 1 0> <0 0 1> 0.004 189.0
YAlO3 (mp-3792) <1 1 0> <0 1 0> 0.009 167.6
DyScO3 (mp-31120) <1 1 0> <1 1 0> 0.012 253.5
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.014 151.2
TbScO3 (mp-31119) <1 1 0> <1 1 0> 0.015 253.5
WSe2 (mp-1821) <1 0 0> <0 0 1> 0.020 50.4
KP(HO2)2 (mp-23959) <0 0 1> <0 1 0> 0.024 301.8
Ge3(BiO3)4 (mp-23560) <1 1 0> <1 0 1> 0.026 160.3
Ge (mp-32) <1 1 0> <0 0 1> 0.026 189.0
ZnO (mp-2133) <1 1 0> <1 0 1> 0.028 120.2
C (mp-66) <1 0 0> <1 1 0> 0.042 50.7
MgF2 (mp-1249) <1 0 1> <0 0 1> 0.056 264.6
Te2W (mp-22693) <0 0 1> <1 0 1> 0.069 200.3
GaAs (mp-2534) <1 1 0> <0 0 1> 0.075 189.0
PbSe (mp-2201) <1 1 1> <0 0 1> 0.076 201.6
GaSb (mp-1156) <1 1 1> <0 0 1> 0.079 201.6
Al (mp-134) <1 1 1> <0 0 1> 0.080 113.4
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.083 239.4
Te2Mo (mp-602) <1 0 1> <0 1 0> 0.087 167.6
KTaO3 (mp-3614) <1 0 0> <0 1 1> 0.088 179.1
CdSe (mp-2691) <1 1 1> <0 0 1> 0.088 201.6
Al (mp-134) <1 0 0> <0 1 1> 0.089 179.1
AlN (mp-661) <1 1 0> <0 1 1> 0.090 107.5
InAs (mp-20305) <1 1 0> <1 0 1> 0.098 160.3
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.099 126.0
GaN (mp-804) <1 1 1> <0 0 1> 0.101 151.2
TiO2 (mp-390) <1 1 1> <0 1 0> 0.104 268.2
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.105 113.4
GdScO3 (mp-5690) <1 1 0> <1 1 0> 0.109 253.5
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.112 152.1
LiAlO2 (mp-3427) <1 0 0> <1 0 1> 0.112 200.3
ZnTe (mp-2176) <1 1 0> <1 0 1> 0.114 160.3
KP(HO2)2 (mp-23959) <0 1 0> <0 1 0> 0.115 301.8
ZnO (mp-2133) <0 0 1> <0 0 1> 0.117 37.8
ZnSe (mp-1190) <1 1 0> <0 0 1> 0.118 189.0
MgF2 (mp-1249) <0 0 1> <0 1 0> 0.125 67.1
C (mp-48) <1 1 1> <0 0 1> 0.128 239.4
ZrO2 (mp-2858) <0 0 1> <0 1 0> 0.133 167.6
SiC (mp-11714) <1 1 0> <0 1 1> 0.133 107.5
KP(HO2)2 (mp-23959) <1 1 1> <1 1 1> 0.139 156.7
CdWO4 (mp-19387) <0 1 0> <0 0 1> 0.143 214.2
TiO2 (mp-390) <1 0 1> <1 0 1> 0.144 40.1
TePb (mp-19717) <1 1 0> <1 0 1> 0.146 120.2
C (mp-66) <1 1 0> <1 0 1> 0.150 160.3
GaSe (mp-1943) <1 0 0> <1 0 1> 0.150 200.3
InSb (mp-20012) <1 0 0> <0 1 0> 0.151 134.1
WS2 (mp-224) <1 0 0> <1 0 1> 0.154 320.5
CdS (mp-672) <0 0 1> <0 0 1> 0.158 201.6
GaSe (mp-1943) <1 0 1> <0 0 1> 0.159 138.6
C (mp-66) <1 1 1> <0 0 1> 0.160 201.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
293 108 134 0 0 0
108 250 93 0 0 0
134 93 268 0 0 0
0 0 0 67 0 0
0 0 0 0 138 0
0 0 0 0 0 66
Compliance Tensor Sij (10-12Pa-1)
4.8 -1.4 -1.9 0 0 0
-1.4 5 -1.1 0 0 0
-1.9 -1.1 5.1 0 0 0
0 0 0 14.8 0 0
0 0 0 0 7.2 0
0 0 0 0 0 15.2
Shear Modulus GV
86 GPa
Bulk Modulus KV
165 GPa
Shear Modulus GR
79 GPa
Bulk Modulus KR
162 GPa
Shear Modulus GVRH
83 GPa
Bulk Modulus KVRH
163 GPa
Elastic Anisotropy
0.42
Poisson's Ratio
0.28

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.10674 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 0.12411 0.00000
0.00000 0.00000 0.00000 0.00000 0.00000 0.04636
Piezoelectric Modulus ‖eijmax
0.05335 C/m2
Crystallographic Direction vmax
1.00000
1.00000
1.00000

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
12
U Values
V: 3.25 eV
Pseudopotentials
VASP PAW: V_pv O F
Final Energy/Atom
-7.1600 eV
Corrected Energy
-95.4575 eV
-95.4575 eV = -85.9203 eV (uncorrected energy) - 6.7280 eV (MP Advanced Correction) - 2.8092 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
User remarks:
  • supplementary compounds from MIT matgen database

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)