Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.072 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.022 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2TiO3 + Li4Ti5O12 + LiNbO3 |
Band Gap2.281 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3 [143] |
HallP 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 297.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 205.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 160.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 365.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 137.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 365.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 342.9 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 274.3 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 68.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 160.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 274.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 182.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 297.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 320.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 342.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 22.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 320.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 251.5 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 160.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 205.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 68.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 114.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 274.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 68.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 205.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 205.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 365.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 274.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 205.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 365.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 68.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 365.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 91.4 |
BN (mp-984) | <1 0 1> | <0 0 1> | 160.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 68.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 22.9 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 297.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 274.3 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 274.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 274.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 365.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 91.4 |
Al (mp-134) | <1 1 1> | <0 0 1> | 205.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 137.2 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 274.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 91.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 205.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 160.0 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 297.2 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 365.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ta24Ti5Se48 (mp-685767) | 0.6279 | 0.156 | 3 |
Li21(Co4O9)2 (mp-850944) | 0.6242 | 0.092 | 3 |
Zn(MoO2)2 (mvc-6112) | 0.6431 | 0.326 | 3 |
Zn(WO2)2 (mvc-6040) | 0.6537 | 0.512 | 3 |
ZnIn2O4 (mp-1094025) | 0.6388 | 0.199 | 3 |
Li3Fe4(OF3)3 (mp-777493) | 0.6021 | 0.173 | 4 |
Li7V(O2F)2 (mp-765256) | 0.6204 | 0.086 | 4 |
Li3Fe4(OF3)3 (mp-776685) | 0.6277 | 0.678 | 4 |
Li2Fe5O5F7 (mp-849531) | 0.6794 | 0.092 | 4 |
Li3Fe4(OF3)3 (mp-780008) | 0.6613 | 0.077 | 4 |
Ti3N4 (mp-1080192) | 0.7368 | 0.100 | 2 |
V2O3 (mp-777698) | 0.6241 | 0.075 | 2 |
V2O3 (mp-776630) | 0.6811 | 0.086 | 2 |
Hf3N4 (mp-776470) | 0.7141 | 0.000 | 2 |
Zr3N4 (mp-277) | 0.7041 | 0.000 | 2 |
Cu6AgBi12PbS22 (mp-651706) | 0.7068 | 0.025 | 5 |
Sr2AlCu2AgO7 (mvc-296) | 0.6789 | 0.118 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ti_pv Nb_pv O |
Final Energy/Atom-7.7881 eV |
Corrected Energy-598.0270 eV
-598.0270 eV = -568.5308 eV (uncorrected energy) - 29.4962 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)