Final Magnetic Moment0.997 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.080 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.060 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCO2 + RuO2 + Na4P2O7 + Ru |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 119.8 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 84.6 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 179.8 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 253.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 309.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 239.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 137.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 209.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 309.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 209.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 179.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 253.8 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 179.8 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 335.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 344.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 335.4 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 241.0 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 59.9 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 299.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 299.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 309.8 |
GaSe (mp-1943) | <1 1 0> | <1 0 0> | 119.8 |
BN (mp-984) | <0 0 1> | <0 1 1> | 236.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 309.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 309.8 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 275.4 |
Al (mp-134) | <1 0 0> | <1 0 1> | 278.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 172.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 34.4 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 1> | 69.7 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 239.7 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 275.4 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 172.1 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 59.9 |
CdTe (mp-406) | <1 1 1> | <1 0 0> | 299.6 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 241.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 241.0 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 239.7 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 172.1 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 295.0 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 59.9 |
C (mp-66) | <1 1 0> | <1 1 1> | 253.8 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 1> | 253.8 |
GdScO3 (mp-5690) | <1 1 0> | <1 1 1> | 253.8 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 275.4 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 34.4 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 309.8 |
KP(HO2)2 (mp-23959) | <1 0 1> | <0 0 1> | 137.7 |
KP(HO2)2 (mp-23959) | <1 1 0> | <0 0 1> | 137.7 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 153.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li9V19O48 (mp-777033) | 0.7356 | 0.102 | 3 |
MgCrPO5 (mvc-3244) | 0.7013 | 0.239 | 4 |
TiZnPO5 (mvc-3128) | 0.6965 | 0.152 | 4 |
MgVPO5 (mvc-3281) | 0.6468 | 0.217 | 4 |
ZnCoPO5 (mvc-3227) | 0.6808 | 0.146 | 4 |
MnZnPO5 (mvc-3247) | 0.6035 | 0.029 | 4 |
Na2TiPCO7 (mp-767550) | 0.1723 | 0.081 | 5 |
Na2CoPCO7 (mp-770988) | 0.1956 | 0.027 | 5 |
Na2VPCO7 (mp-770717) | 0.2027 | 0.000 | 5 |
Na2CrPCO7 (mp-769616) | 0.1663 | 0.000 | 5 |
Na2GePCO7 (mp-768132) | 0.2086 | 0.093 | 5 |
Na2LiMnPCO7 (mp-764273) | 0.6622 | 0.084 | 6 |
Li6FeNiP2(CO7)2 (mp-767289) | 0.6981 | 0.041 | 6 |
NaLiMnPCO7 (mp-763833) | 0.5904 | 0.062 | 6 |
Na5LiNi2P2(CO7)2 (mp-770324) | 0.6776 | 0.009 | 6 |
CuP2H8CN2O5 (mp-24145) | 0.6486 | 0.288 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv P Ru_pv C O |
Final Energy/Atom-6.7685 eV |
Corrected Energy-172.0626 eV
Uncorrected energy = -162.4446 eV
Composition-based energy adjustment (-0.687 eV/atom x 14.0 atoms) = -9.6180 eV
Corrected energy = -172.0626 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)