Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.476 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.98 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.386 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 79.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 197.8 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 356.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 118.7 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 184.6 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 143.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 277.0 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 320.4 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 123.0 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 307.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 316.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 197.8 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 142.4 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 251.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 64.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 79.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 193.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 277.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 251.0 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 267.0 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 286.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 107.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 64.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 71.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 -1> | 221.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 128.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 184.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 64.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 358.6 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 251.0 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 251.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 64.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 184.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 184.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 197.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 184.6 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 251.0 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 237.4 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 251.0 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 257.6 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 158.3 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 179.3 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 197.8 |
YVO4 (mp-19133) | <0 0 1> | <1 0 -1> | 257.6 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 320.4 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 267.0 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 246.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 316.5 |
Te2W (mp-22693) | <1 0 0> | <1 1 -1> | 294.8 |
TePb (mp-19717) | <1 0 0> | <1 1 -1> | 221.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn2PO5 (mp-770538) | 0.6067 | 0.004 | 3 |
LiMn2F5 (mp-777631) | 0.5893 | 0.069 | 3 |
Cr5(PO4)4 (mp-540446) | 0.5665 | 0.007 | 3 |
LiFe2F5 (mp-776933) | 0.6517 | 0.070 | 3 |
Cr5(PO4)4 (mp-775246) | 0.5661 | 0.007 | 3 |
Li3Cr2(PO4)3 (mp-775597) | 0.5287 | 0.005 | 4 |
Li2Cr2P2O9 (mp-761438) | 0.4962 | 0.079 | 4 |
Li2V(PO4)2 (mp-540312) | 0.5146 | 0.056 | 4 |
LiCrPO5 (mp-850227) | 0.5180 | 0.065 | 4 |
Li2Co2P2O9 (mp-761973) | 0.4798 | 0.081 | 4 |
Li2VP2HO8 (mp-780754) | 0.0485 | 0.001 | 5 |
LiMn2P2HO8 (mp-779995) | 0.4603 | 0.036 | 5 |
LiFe2P2HO8 (mp-773622) | 0.4358 | 0.035 | 5 |
Li4Ni2P4H3O16 (mp-850115) | 0.4406 | 0.054 | 5 |
Li2MnP2HO8 (mp-781059) | 0.2790 | 0.005 | 5 |
Li4TiNi3Sn2(PO4)6 (mp-778249) | 0.6285 | 0.054 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P H O |
Final Energy/Atom-6.5894 eV |
Corrected Energy-402.4140 eV
-402.4140 eV = -369.0087 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)