Final Magnetic Moment24.961 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.904 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.24 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Si2O5 + LiScSiO4 + Fe2O3 + SiO2 |
Band Gap2.750 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 287.2 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 170.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 307.0 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 170.7 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 170.7 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 215.4 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 230.2 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 307.0 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 223.8 |
TePb (mp-19717) | <1 0 0> | <0 1 1> | 85.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 254.2 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 215.4 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 223.8 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 287.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 245.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 307.0 |
BN (mp-984) | <1 1 1> | <0 0 1> | 245.6 |
MoS2 (mp-1434) | <1 0 1> | <1 0 0> | 205.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 1> | 256.0 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 184.2 |
CdTe (mp-406) | <1 0 0> | <0 1 1> | 85.3 |
LiTaO3 (mp-3666) | <1 1 1> | <0 1 1> | 256.0 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 307.0 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 307.0 |
C (mp-66) | <1 0 0> | <0 0 1> | 307.0 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 307.0 |
TiO2 (mp-2657) | <0 0 1> | <0 1 1> | 85.3 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 307.0 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 307.0 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 215.4 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 307.0 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 307.0 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 215.4 |
Mg (mp-153) | <1 0 1> | <0 1 1> | 170.7 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 245.6 |
GaP (mp-2490) | <1 1 0> | <0 1 0> | 287.2 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 245.6 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 307.0 |
Ni (mp-23) | <1 0 0> | <1 -1 0> | 136.0 |
InSb (mp-20012) | <1 0 0> | <0 1 1> | 85.3 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 184.2 |
NdGaO3 (mp-3196) | <0 1 0> | <0 1 0> | 287.2 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 307.0 |
SiC (mp-11714) | <0 0 1> | <0 1 0> | 287.2 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 307.0 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 307.0 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 1> | 256.0 |
Si (mp-149) | <1 1 0> | <0 1 0> | 287.2 |
WS2 (mp-224) | <1 0 0> | <1 0 1> | 223.8 |
C (mp-48) | <0 0 1> | <1 0 0> | 205.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg17(SiO3)16 (mp-757674) | 0.4194 | 0.112 | 3 |
MgSiO3 (mp-5026) | 0.3826 | 0.007 | 3 |
CdSiO3 (mp-776023) | 0.2414 | 0.027 | 3 |
NaVO3 (mp-19083) | 0.4322 | 0.000 | 3 |
MnSiO3 (mp-25041) | 0.3535 | 0.016 | 3 |
LiGa(SiO3)2 (mp-6745) | 0.1572 | 0.041 | 4 |
LiCo(SiO3)2 (mp-767356) | 0.1481 | 0.063 | 4 |
LiFe(SiO3)2 (mp-510708) | 0.1186 | 0.008 | 4 |
LiV(SiO3)2 (mp-19043) | 0.1585 | 0.002 | 4 |
LiFe(SiO3)2 (mp-559892) | 0.1088 | 0.008 | 4 |
MoO2 (mvc-6944) | 0.6747 | 0.281 | 2 |
Li8Sc5Fe3(SiO3)16 (mp-775186) | 0.1787 | 0.004 | 5 |
Li5Sc2Fe3(SiO3)10 (mp-775172) | 0.0968 | 0.005 | 5 |
Li2ScFe(SiO3)4 (mp-772338) | 0.0684 | 0.007 | 5 |
Li4ScFe3(SiO3)8 (mp-767448) | 0.0395 | 0.217 | 5 |
Li8ScFe7(SiO3)16 (mp-775203) | 0.0363 | 0.005 | 5 |
NaCa3ScZn3(SiO3)8 (mp-693463) | 0.6129 | 0.029 | 6 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.5711 | 0.080 | 6 |
NaCaScZn(SiO3)4 (mp-684991) | 0.6019 | 0.019 | 6 |
NaCa2ScZn2(SiO3)6 (mp-534778) | 0.6021 | 0.025 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.5635 | 0.020 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Sc_sv Fe_pv Si O |
Final Energy/Atom-7.3108 eV |
Corrected Energy-477.5981 eV
-477.5981 eV = -438.6506 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction) - 13.6650 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)