Final Magnetic Moment9.006 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.476 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.089 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCr5O12 + LiCrP2O7 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 78.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 312.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 137.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 156.3 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 190.2 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 234.5 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 209.1 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 277.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 146.6 |
TeO2 (mp-2125) | <0 1 0> | <1 0 -1> | 137.9 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 208.4 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 208.4 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 234.5 |
Mg (mp-153) | <1 0 1> | <1 1 0> | 209.1 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 156.3 |
LaF3 (mp-905) | <0 0 1> | <1 0 0> | 312.7 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 146.6 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 78.2 |
SiC (mp-11714) | <0 0 1> | <0 1 0> | 208.4 |
SiC (mp-11714) | <1 0 0> | <0 1 0> | 277.9 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 312.7 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 234.5 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 209.1 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 156.3 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 234.5 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 0> | 277.9 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 78.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 146.6 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 78.2 |
Au (mp-81) | <1 0 0> | <1 0 0> | 156.3 |
Au (mp-81) | <1 1 0> | <0 0 1> | 146.6 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 190.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 156.3 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 78.2 |
BN (mp-984) | <0 0 1> | <1 0 0> | 234.5 |
C (mp-48) | <0 0 1> | <0 1 0> | 277.9 |
WSe2 (mp-1821) | <0 0 1> | <0 1 0> | 277.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 146.6 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 137.9 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 156.3 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 312.7 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 234.5 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 312.7 |
SiC (mp-7631) | <1 0 0> | <1 0 1> | 190.2 |
CaCO3 (mp-3953) | <1 0 1> | <0 1 0> | 277.9 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 146.6 |
YAlO3 (mp-3792) | <1 1 1> | <1 0 0> | 312.7 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 156.3 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 78.2 |
CdWO4 (mp-19387) | <0 0 1> | <0 1 0> | 208.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Co3(P2O7)2 (mvc-12220) | 0.4006 | 0.025 | 3 |
Ni3(P2O7)2 (mvc-11990) | 0.3753 | 0.060 | 3 |
Cr3(P2O7)2 (mp-540180) | 0.4001 | 0.038 | 3 |
Ni3(P2O7)2 (mp-32394) | 0.3779 | 0.060 | 3 |
Cr3(P2O7)2 (mp-775249) | 0.3980 | 0.038 | 3 |
LiFeP2O7 (mp-763683) | 0.4115 | 0.074 | 4 |
LiVP2O7 (mp-763409) | 0.3939 | 0.065 | 4 |
LiMn2(PO4)3 (mp-32012) | 0.3201 | 0.082 | 4 |
LiNi2(PO4)3 (mp-32337) | 0.2610 | 0.157 | 4 |
LiCr2(PO4)3 (mp-31646) | 0.3323 | 0.108 | 4 |
FeO2 (mvc-11999) | 0.6407 | 0.372 | 2 |
CrO2 (mvc-11581) | 0.5113 | 0.166 | 2 |
VO2 (mp-777469) | 0.6262 | 0.038 | 2 |
VO2 (mvc-6918) | 0.5119 | 0.094 | 2 |
MoO2 (mvc-6944) | 0.5946 | 0.281 | 2 |
LiMnPO4F (mp-762774) | 0.5244 | 0.320 | 5 |
Li2VSO4F3 (mp-769602) | 0.4914 | 0.087 | 5 |
K2CoP2WO10 (mp-645301) | 0.5558 | 0.000 | 5 |
K2Mn2P2O7F2 (mp-566013) | 0.4808 | 0.000 | 5 |
LiMn2P2HO9 (mp-780931) | 0.5680 | 0.030 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.6363 | 0.255 | 6 |
Na2Gd2MgSi4(O6F)2 (mp-557538) | 0.6722 | 0.000 | 6 |
NaLiMn2Fe4(PO4)6 (mp-777193) | 0.4868 | 0.021 | 6 |
Na5CaAl5Fe(SiO3)12 (mp-744927) | 0.6772 | 0.034 | 6 |
Mn4Si4SnB2(HO9)2 (mp-743890) | 0.6440 | 0.000 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.7165 | 0.002 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv P O |
Final Energy/Atom-7.0882 eV |
Corrected Energy-287.1711 eV
-287.1711 eV = -262.2642 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 8.0520 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)