Final Magnetic Moment12.989 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.427 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.061 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.71 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiV(CO3)2 + Li3V2(PO4)3 + FeCO3 + V2O3 + Li3PO4 + C |
Band Gap2.710 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm [6] |
HallP 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 0> | <0 0 1> | 168.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 330.4 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 280.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 330.4 |
AlN (mp-661) | <1 0 0> | <1 1 -1> | 236.6 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 330.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 165.4 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 169.2 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 247.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 165.4 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 336.0 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 132.1 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 264.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 280.0 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 180.7 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 330.4 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 280.0 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 271.0 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 280.0 |
BN (mp-984) | <0 0 1> | <1 0 1> | 180.7 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 330.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 168.0 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 1> | 180.7 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 330.4 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 180.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 336.0 |
BN (mp-984) | <1 0 1> | <1 0 0> | 264.3 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 224.0 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 224.0 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 280.0 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 336.0 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 202.9 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 66.1 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 198.2 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 280.0 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 132.1 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 253.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 264.3 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 330.4 |
C (mp-66) | <1 1 0> | <1 0 0> | 330.4 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 198.2 |
C (mp-66) | <1 0 0> | <1 0 -1> | 165.4 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 168.0 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 336.0 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 330.4 |
Mg (mp-153) | <0 0 1> | <0 1 1> | 202.9 |
Mg (mp-153) | <1 0 1> | <1 1 1> | 247.5 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 330.4 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 330.4 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 198.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3Fe3(BO3)4 (mp-767662) | 0.6598 | 0.088 | 4 |
Li3Si2Bi3O10 (mp-757200) | 0.7346 | 0.053 | 4 |
Li9V12Te7O48 (mp-849282) | 0.7006 | 0.058 | 4 |
Na3Ca(BO2)5 (mp-614628) | 0.7378 | 0.002 | 4 |
Li3Ni(BO2)5 (mp-771081) | 0.7411 | 0.061 | 4 |
Li3CoPCO7 (mp-767912) | 0.1932 | 0.173 | 5 |
Li3VPCO7 (mp-767894) | 0.1206 | 0.085 | 5 |
Li3NiPCO7 (mp-767883) | 0.1692 | 0.052 | 5 |
Li3VPCO7 (mp-767879) | 0.2065 | 0.083 | 5 |
Li3NiPCO7 (mp-767869) | 0.2201 | 0.055 | 5 |
Li12MnV3P4(CO7)4 (mp-861700) | 0.0733 | 0.068 | 6 |
Li12VFe3P4(CO7)4 (mp-767730) | 0.0618 | 0.047 | 6 |
Li6VCoP2(CO7)2 (mp-767294) | 0.0449 | 0.056 | 6 |
Li6VFeP2(CO7)2 (mp-767284) | 0.0899 | 0.055 | 6 |
Li6MnVP2(CO7)2 (mp-767281) | 0.0843 | 0.095 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Fe_pv P C O |
Final Energy/Atom-6.8170 eV |
Corrected Energy-381.9250 eV
-381.9250 eV = -354.4819 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 7.7790 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)