Final Magnetic Moment8.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.343 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.076 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnO2 + Li2O + LiF |
Band Gap0.814 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 1> | 277.6 |
AlN (mp-661) | <1 0 0> | <1 -1 0> | 175.1 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 180.1 |
AlN (mp-661) | <1 1 1> | <1 -1 -1> | 257.2 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 227.8 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 277.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 210.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 150.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 330.8 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 295.4 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 287.5 |
KCl (mp-23193) | <1 1 0> | <1 1 -1> | 293.4 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 196.9 |
BaF2 (mp-1029) | <1 1 0> | <1 1 -1> | 293.4 |
GaN (mp-804) | <0 0 1> | <1 -1 -1> | 257.2 |
GaN (mp-804) | <1 0 1> | <1 -1 -1> | 192.9 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 208.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 215.7 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 284.8 |
InAs (mp-20305) | <1 1 0> | <1 -1 -1> | 321.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 330.8 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 227.8 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 295.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 270.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 -1> | 183.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 -1> | 305.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 -1> | 183.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 330.8 |
CdS (mp-672) | <1 0 0> | <1 -1 -1> | 257.2 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 230.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 240.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 113.9 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 284.8 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 98.5 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 284.8 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 284.8 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 284.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 240.2 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 270.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 150.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 270.7 |
Te2Mo (mp-602) | <1 1 0> | <0 1 0> | 284.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 90.2 |
TePb (mp-19717) | <1 1 0> | <1 1 -1> | 293.4 |
Te2Mo (mp-602) | <1 0 0> | <0 1 1> | 270.6 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 90.2 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 203.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 180.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 287.5 |
BN (mp-984) | <0 0 1> | <1 -1 1> | 268.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li4Mn5O10 (mp-763777) | 0.3483 | 0.052 | 3 |
Li2Mn3O6 (mp-762409) | 0.3820 | 0.069 | 3 |
Li9Mn10O20 (mp-780186) | 0.3413 | 0.039 | 3 |
Li6W2O9 (mp-767923) | 0.3824 | 0.055 | 3 |
Li8Nb2O9 (mp-28030) | 0.3347 | 0.000 | 3 |
Li6Mn2O5F2 (mp-767468) | 0.2937 | 0.079 | 4 |
Li4Mn3(SnO5)2 (mp-763667) | 0.2782 | 0.433 | 4 |
Li6Fe2O5F2 (mp-777253) | 0.2814 | 0.308 | 4 |
Li4V3Cr2O10 (mp-780925) | 0.3328 | 0.075 | 4 |
Li4Mn5(CuO6)2 (mp-849516) | 0.3258 | 0.195 | 4 |
Ni6O7 (mp-767815) | 0.6040 | 0.047 | 2 |
Ni5O6 (mp-782702) | 0.5204 | 0.041 | 2 |
Fe15O16 (mp-705551) | 0.5720 | 0.077 | 2 |
Ni5Cl6 (mp-1094110) | 0.4661 | 0.332 | 2 |
Ni6Cl7 (mp-1022720) | 0.6031 | 0.376 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.4867 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv O F |
Final Energy/Atom-5.7088 eV |
Corrected Energy-185.0091 eV
-185.0091 eV = -171.2628 eV (uncorrected energy) - 7.0229 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)