Final Magnetic Moment0.546 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.334 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.172 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.69 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi11V8(PO4)12 + LiV(CO3)2 + V2O3 + Li3PO4 + C |
Band Gap0.607 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 168.9 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 330.1 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 166.0 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 169.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 168.9 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 213.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 337.7 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 330.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 330.1 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 166.0 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 337.7 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 198.1 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 249.1 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 202.4 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 132.0 |
TePb (mp-19717) | <1 1 0> | <0 1 1> | 249.1 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 330.1 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 281.5 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 264.1 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 249.1 |
BN (mp-984) | <1 0 0> | <0 0 1> | 337.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 168.9 |
BN (mp-984) | <1 0 1> | <0 1 0> | 264.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 66.0 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 249.1 |
MoS2 (mp-1434) | <0 0 1> | <1 0 1> | 202.4 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 281.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 330.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 330.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 198.1 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 330.1 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 132.0 |
CdTe (mp-406) | <1 1 0> | <0 1 1> | 249.1 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 253.8 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 337.7 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 225.2 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 264.1 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 330.1 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 198.1 |
C (mp-66) | <1 1 0> | <0 0 1> | 281.5 |
GdScO3 (mp-5690) | <0 1 1> | <0 1 0> | 330.1 |
C (mp-66) | <1 0 0> | <0 1 1> | 166.0 |
Mg (mp-153) | <0 0 1> | <1 0 1> | 202.4 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 337.7 |
Mg (mp-153) | <1 0 1> | <1 1 -1> | 246.8 |
LaF3 (mp-905) | <1 0 0> | <0 1 0> | 330.1 |
InP (mp-20351) | <1 1 0> | <0 1 1> | 249.1 |
TbScO3 (mp-31119) | <0 1 1> | <0 1 0> | 330.1 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 198.1 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 281.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3Fe3(BO3)4 (mp-767662) | 0.6608 | 0.362 | 4 |
Li9V12Te7O48 (mp-849282) | 0.6595 | 0.057 | 4 |
Li3V(BO2)5 (mp-770344) | 0.7161 | 0.111 | 4 |
Na3Ca(BO2)5 (mp-614628) | 0.6983 | 0.002 | 4 |
Li3Ni(BO2)5 (mp-771081) | 0.7038 | 0.092 | 4 |
Li3VPCO7 (mp-861720) | 0.1679 | 0.277 | 5 |
Li3CoPCO7 (mp-767928) | 0.2278 | 0.187 | 5 |
Li3CoPCO7 (mp-767912) | 0.2052 | 0.173 | 5 |
Li3VPCO7 (mp-767894) | 0.1375 | 0.153 | 5 |
Li3NiPCO7 (mp-767883) | 0.1773 | 0.096 | 5 |
Li12V3CrP4(CO7)4 (mp-767729) | 0.1850 | 0.069 | 6 |
Li12MnNi3P4(CO7)4 (mp-767698) | 0.1704 | 0.040 | 6 |
Li12MnV3P4(CO7)4 (mp-861700) | 0.1665 | 0.171 | 6 |
Li6MnNiP2(CO7)2 (mp-767293) | 0.1921 | 0.046 | 6 |
Li6MnVP2(CO7)2 (mp-767281) | 0.1763 | 0.095 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P C O |
Final Energy/Atom-6.7560 eV |
Corrected Energy-377.7035 eV
-377.7035 eV = -351.3114 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)