Final Magnetic Moment10.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.731 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.635 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 211.0 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 233.7 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 201.9 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 252.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 119.3 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 175.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 211.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 263.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 316.5 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 151.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 252.4 |
SiO2 (mp-6930) | <1 0 1> | <1 1 -1> | 308.8 |
SiO2 (mp-6930) | <1 1 1> | <1 1 -1> | 154.4 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 211.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 219.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 175.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 -1> | 175.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 233.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 311.0 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 0> | 278.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 211.0 |
MgO (mp-1265) | <1 0 0> | <1 0 -1> | 233.7 |
MgO (mp-1265) | <1 1 0> | <1 0 -1> | 233.7 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 211.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 302.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 302.9 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 263.7 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 233.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 158.2 |
CdS (mp-672) | <1 0 0> | <1 1 -1> | 308.8 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 233.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 316.5 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 302.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 211.0 |
C (mp-66) | <1 0 0> | <0 1 1> | 292.0 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 292.0 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 1> | 219.0 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 -1> | 175.2 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 263.7 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 233.3 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 311.0 |
GdScO3 (mp-5690) | <1 1 1> | <0 1 0> | 151.4 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 311.0 |
Mg (mp-153) | <0 0 1> | <1 1 -1> | 308.8 |
Mg (mp-153) | <1 0 0> | <0 1 1> | 219.0 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 151.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 263.7 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 316.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 211.0 |
Ag (mp-124) | <1 0 0> | <1 1 -1> | 154.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiClO4 (mp-30301) | 0.5326 | 0.000 | 3 |
CuSO4 (mp-20525) | 0.5293 | 0.000 | 3 |
MnPO4 (mp-777460) | 0.5516 | 0.000 | 3 |
CoPO4 (mp-777025) | 0.5471 | 0.135 | 3 |
Mn4(PO4)3 (mp-32010) | 0.5587 | 0.142 | 3 |
LiSnP2O7 (mp-759068) | 0.5106 | 0.095 | 4 |
LiMn3(PO4)3 (mp-771361) | 0.4921 | 0.114 | 4 |
LiBi2P3O11 (mp-758810) | 0.5041 | 0.082 | 4 |
Al4P3(HO5)3 (mp-706709) | 0.4583 | 0.027 | 4 |
Fe4P3(HO5)3 (mp-25756) | 0.4199 | 0.000 | 4 |
Cr5O12 (mp-19575) | 0.6655 | 0.142 | 2 |
Fe2CuAs2(HO5)2 (mp-764827) | 0.5132 | 0.283 | 5 |
LiMnHSO5 (mp-943469) | 0.6232 | 0.278 | 5 |
LiMn3P2(HO3)4 (mp-763726) | 0.6366 | 0.479 | 5 |
NaAl3P2(HO3)4 (mp-706525) | 0.5768 | 0.006 | 5 |
ZnCoPHO5 (mp-603567) | 0.6363 | 0.000 | 5 |
LiMnVP2(HO5)2 (mp-765066) | 0.6131 | 0.143 | 6 |
LiMnVP2(HO5)2 (mp-765378) | 0.5948 | 0.046 | 6 |
LiMnVP2(HO5)2 (mp-766999) | 0.6418 | 0.039 | 6 |
LiMnVP2(HO5)2 (mp-765324) | 0.5303 | 0.072 | 6 |
LiMnVP2(HO5)2 (mp-765103) | 0.6150 | 0.039 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Zn Fe_pv As H O |
Final Energy/Atom-5.9071 eV |
Corrected Energy-225.8205 eV