Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.159 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.064 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.94 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiVF4 + LiF |
Band Gap2.566 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 112.1 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 261.7 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 112.1 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 299.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 336.4 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 299.1 |
GaN (mp-804) | <1 0 1> | <1 1 -1> | 264.2 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 112.1 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 239.6 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 112.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 336.4 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 112.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 186.9 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 299.1 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 239.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 263.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 263.3 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 112.1 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 149.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 261.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 70.6 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 186.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 149.5 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 210.6 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 239.6 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 112.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 263.3 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 112.1 |
InAs (mp-20305) | <1 1 1> | <1 1 -1> | 264.2 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 159.8 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 141.2 |
YVO4 (mp-19133) | <1 1 0> | <1 0 -1> | 263.3 |
TePb (mp-19717) | <1 0 0> | <1 0 -1> | 210.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 210.6 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 261.7 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 149.5 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 263.3 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 112.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 212.6 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 149.5 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 74.8 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 149.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 159.4 |
BN (mp-984) | <1 1 0> | <1 1 -1> | 264.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 224.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 336.4 |
GaSe (mp-1943) | <1 0 0> | <1 1 1> | 206.4 |
BN (mp-984) | <0 0 1> | <1 0 0> | 224.3 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 158.0 |
BN (mp-984) | <1 1 1> | <1 0 0> | 336.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.27 | 0.00 | 0.03 |
0.00 | 2.34 | 0.00 |
0.03 | 0.00 | 2.25 |
Dielectric Tensor εij (total) |
||
---|---|---|
7.06 | 0.00 | 0.64 |
0.00 | 7.29 | 0.00 |
0.64 | 0.00 | 7.97 |
Polycrystalline dielectric constant
εpoly∞
2.29
|
Polycrystalline dielectric constant
εpoly
7.44
|
Refractive Index n1.51 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Gd2HfO5 (mp-755251) | 0.2992 | 0.051 | 3 |
TiGa2O5 (mp-752733) | 0.3001 | 0.077 | 3 |
Li2MnF5 (mp-556229) | 0.3085 | 0.209 | 3 |
Y2HfO5 (mp-753917) | 0.2563 | 0.029 | 3 |
Li2MnF5 (mp-621395) | 0.2981 | 0.209 | 3 |
LiV6O7F5 (mp-777058) | 0.4253 | 0.097 | 4 |
Ta2TiZn2O8 (mvc-2345) | 0.4203 | 0.159 | 4 |
Ta2Zn2NiO8 (mvc-2670) | 0.4116 | 0.008 | 4 |
Ta2Zn2CoO8 (mvc-2669) | 0.4222 | 0.024 | 4 |
TiNb2Zn2O8 (mvc-3345) | 0.4302 | 0.120 | 4 |
Ti6O11 (mp-30524) | 0.3805 | 0.012 | 2 |
Ti5O9 (mp-748) | 0.3831 | 0.011 | 2 |
Ti6O11 (mp-680568) | 0.3975 | 0.012 | 2 |
V5O9 (mp-704305) | 0.3572 | 0.008 | 2 |
Ti5O9 (mp-554715) | 0.3850 | 0.011 | 2 |
Li4FeTe(WO6)2 (mp-771716) | 0.4475 | 0.163 | 5 |
Li4MnSb(WO6)2 (mp-779994) | 0.4545 | 0.041 | 5 |
Li4MnSb2WO12 (mp-763536) | 0.4694 | 0.068 | 5 |
Li4NbFe(TeO6)2 (mp-776914) | 0.4607 | 0.030 | 5 |
Li4VFe(WO6)2 (mp-761519) | 0.4587 | 0.070 | 5 |
Run TypeGGA+U |
Energy Cutoff700 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv F |
Final Energy/Atom-5.4495 eV |
Corrected Energy-90.5566 eV
-90.5566 eV = -87.1926 eV (uncorrected energy) - 3.3640 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)