Final Magnetic Moment16.995 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.357 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.068 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFeP2O7 + Li4P2O7 + FePO4 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 271.7 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 162.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 319.2 |
CeO2 (mp-20194) | <1 1 1> | <1 -1 -1> | 258.1 |
BaF2 (mp-1029) | <1 0 0> | <0 1 -1> | 281.3 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 233.5 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 271.7 |
GaN (mp-804) | <1 0 0> | <1 -1 0> | 237.3 |
GaN (mp-804) | <1 0 1> | <1 -1 -1> | 172.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 266.0 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 311.3 |
SiO2 (mp-6930) | <1 1 0> | <1 -1 0> | 237.3 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 155.6 |
KCl (mp-23193) | <1 0 0> | <0 1 -1> | 281.3 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 233.5 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 271.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 326.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 -1> | 281.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 266.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 227.5 |
CdS (mp-672) | <1 0 0> | <1 -1 0> | 237.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 266.0 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 217.4 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 263.4 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 131.7 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 271.7 |
YVO4 (mp-19133) | <1 1 0> | <1 -1 -1> | 258.1 |
TePb (mp-19717) | <1 1 0> | <1 0 -1> | 233.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 266.0 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 271.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 -1 0> | 237.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 319.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 266.0 |
BN (mp-984) | <1 0 1> | <1 0 0> | 303.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 266.0 |
BN (mp-984) | <1 1 1> | <0 0 1> | 266.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 266.0 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 319.2 |
MoS2 (mp-1434) | <1 0 0> | <0 1 0> | 271.7 |
MoS2 (mp-1434) | <1 0 1> | <0 1 0> | 271.7 |
GaP (mp-2490) | <1 1 1> | <1 -1 -1> | 258.1 |
Al (mp-134) | <1 0 0> | <0 1 0> | 217.4 |
Al (mp-134) | <1 1 0> | <1 0 0> | 227.5 |
LiGaO2 (mp-5854) | <0 1 0> | <1 -1 -1> | 258.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 217.4 |
CdTe (mp-406) | <1 1 0> | <1 -1 -1> | 258.1 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 326.0 |
TbScO3 (mp-31119) | <1 0 1> | <0 1 -1> | 281.3 |
TeO2 (mp-2125) | <0 0 1> | <0 1 1> | 162.7 |
InSb (mp-20012) | <1 1 0> | <1 -1 -1> | 258.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe3(P2O7)2 (mvc-12221) | 0.5123 | 0.327 | 3 |
Mn7(P2O7)4 (mp-779406) | 0.4778 | 0.000 | 3 |
V3(P2O7)2 (mp-32416) | 0.5202 | 0.033 | 3 |
Fe3(P2O7)2 (mp-540486) | 0.5008 | 0.327 | 3 |
Mn4(PO4)3 (mp-32010) | 0.4956 | 0.142 | 3 |
Li2V(PO4)2 (mp-705365) | 0.4139 | 0.063 | 4 |
Li3Mn4(PO4)6 (mp-767568) | 0.3532 | 0.054 | 4 |
ZnFe3(P2O7)2 (mvc-901) | 0.4025 | 0.391 | 4 |
Li3Cr4(PO4)6 (mp-767848) | 0.3255 | 0.052 | 4 |
Li3V4(PO4)6 (mp-767790) | 0.2391 | 0.062 | 4 |
CrO2 (mvc-11581) | 0.7426 | 0.166 | 2 |
VO2 (mvc-6918) | 0.6970 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.6735 | 0.281 | 2 |
NaLi7Fe8(SiO3)16 (mp-775490) | 0.5476 | 0.158 | 5 |
Li2MnV(PO4)3 (mp-771372) | 0.5802 | 0.240 | 5 |
Li2MnV(PO4)3 (mp-770179) | 0.5795 | 0.039 | 5 |
LiMnV(PO4)3 (mp-770143) | 0.5648 | 0.104 | 5 |
LiMn2P2HO9 (mp-780931) | 0.5558 | 0.144 | 5 |
LiMnVP2(HO5)2 (mp-765066) | 0.6391 | 0.143 | 6 |
LiMnVP2(HO5)2 (mp-765378) | 0.6415 | 0.046 | 6 |
LiMnVP2(HO5)2 (mp-766999) | 0.6513 | 0.039 | 6 |
NaLiMn2Fe4(PO4)6 (mp-777193) | 0.4743 | 0.018 | 6 |
LiMnVP2(HO5)2 (mp-765324) | 0.6092 | 0.072 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6299 | 0.068 | 7 |
KNa2LiTi2Fe2(SiO3)8 (mp-542926) | 0.7138 | 0.071 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P O |
Final Energy/Atom-6.7634 eV |
Corrected Energy-278.0326 eV
-278.0326 eV = -250.2456 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)