Final Magnetic Moment7.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.298 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoPO4 + LiCoPO4 |
Band Gap0.671 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <0 0 1> | <0 0 1> | 218.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 131.2 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 86.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 43.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 87.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 218.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 306.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 349.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 306.0 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 173.8 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 172.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 43.7 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 266.3 |
BN (mp-984) | <1 1 1> | <0 0 1> | 131.2 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 218.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 306.0 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 349.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 131.2 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 349.7 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 218.6 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 218.6 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 218.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 131.2 |
C (mp-66) | <1 1 0> | <0 0 1> | 131.2 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 349.7 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 1> | 173.8 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 131.2 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 86.3 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 218.6 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 306.0 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 349.7 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 306.0 |
PbSe (mp-2201) | <1 1 1> | <1 0 -1> | 266.3 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 0> | 163.7 |
BaTiO3 (mp-5986) | <1 1 0> | <1 1 -1> | 165.1 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 -1> | 266.3 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 349.7 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 349.7 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 172.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 349.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 218.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 131.2 |
InAs (mp-20305) | <1 1 1> | <1 0 -1> | 266.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 218.6 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 131.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 262.3 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 266.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 262.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 262.3 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 208.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Be2P2O7 (mp-779622) | 0.6555 | 0.084 | 3 |
Be2P2O7 (mp-779108) | 0.6288 | 0.019 | 3 |
LiPO3 (mp-557189) | 0.4509 | 0.001 | 3 |
Fe3(SiO4)2 (mp-850744) | 0.3906 | 0.104 | 3 |
Li2Si3O7 (mp-555899) | 0.6653 | 0.002 | 3 |
Li2Fe(PO4)2 (mp-762755) | 0.3351 | 0.243 | 4 |
LiMn2(PO4)2 (mp-767855) | 0.2879 | 0.058 | 4 |
LiFe2(PO4)2 (mp-767221) | 0.3972 | 0.200 | 4 |
Li2Fe(PO4)2 (mp-31815) | 0.3865 | 0.278 | 4 |
LiNi2(PO4)2 (mp-768319) | 0.2137 | 0.091 | 4 |
Zn2P2HNO8 (mp-707891) | 0.6215 | 0.533 | 5 |
SrAl2SiN2O3 (mp-554390) | 0.7191 | 0.003 | 5 |
Cs2Li2B2P4O15 (mp-1019606) | 0.5902 | 0.000 | 5 |
LiCu2P3(HO5)2 (mp-849424) | 0.6942 | 0.071 | 5 |
RbZn2P2HO8 (mp-24683) | 0.6486 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co P O |
Final Energy/Atom-6.6956 eV |
Corrected Energy-385.6347 eV
-385.6347 eV = -348.1694 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 14.9920 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)