Final Magnetic Moment0.217 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.423 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.150 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnPO4 + MnO2 + LiPO3 + O2 |
Band Gap0.827 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 281.6 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 244.2 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 298.4 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 140.8 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 125.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 281.6 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 281.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 140.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 281.6 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 298.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 205.4 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 122.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 70.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 244.2 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 102.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 211.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 140.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 281.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 250.1 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 99.5 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 143.0 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 281.6 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 99.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 1> | 122.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 281.6 |
Al (mp-134) | <1 1 0> | <1 0 0> | 205.4 |
Al (mp-134) | <1 1 1> | <1 0 1> | 250.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 211.2 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 244.2 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 281.6 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 198.9 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 205.4 |
TeO2 (mp-2125) | <1 1 0> | <0 1 0> | 99.5 |
TeO2 (mp-2125) | <1 1 1> | <0 0 1> | 211.2 |
SiC (mp-7631) | <1 1 0> | <0 1 1> | 244.2 |
Fe3O4 (mp-19306) | <1 0 0> | <1 1 0> | 143.0 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 0> | 102.7 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 281.6 |
C (mp-66) | <1 1 0> | <0 1 0> | 198.9 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 281.6 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 140.8 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 140.8 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 198.9 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 281.6 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 298.4 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 140.8 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 102.7 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 281.6 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 70.4 |
PbS (mp-21276) | <1 1 1> | <0 1 1> | 122.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni7(P2O7)4 (mp-779819) | 0.4808 | 0.019 | 3 |
Cr5(PO4)4 (mp-540446) | 0.4392 | 0.007 | 3 |
Cr4Si4O13 (mp-768078) | 0.5031 | 0.139 | 3 |
Cr5(PO4)4 (mp-775246) | 0.4420 | 0.007 | 3 |
Mn5(P3O11)2 (mp-31954) | 0.4645 | 0.065 | 3 |
Li3Cr4(PO4)6 (mp-768047) | 0.3163 | 0.222 | 4 |
Li2Mn2(PO4)3 (mp-774345) | 0.2869 | 0.029 | 4 |
LiMn2(PO4)3 (mp-32004) | 0.3555 | 0.023 | 4 |
Li2Mn2(PO4)3 (mp-762743) | 0.3716 | 0.017 | 4 |
Li3Mn4(PO4)6 (mp-767957) | 0.3126 | 0.020 | 4 |
LiMn2P2(O4F)2 (mp-763273) | 0.4511 | 0.480 | 5 |
Li2MnV(PO4)3 (mp-779088) | 0.3957 | 0.036 | 5 |
Li6MnV3(PO4)6 (mp-778914) | 0.4475 | 0.228 | 5 |
LiMgAl3(SeO4)6 (mp-532676) | 0.4530 | 0.010 | 5 |
LiMnPO4F (mp-763235) | 0.4686 | 0.567 | 5 |
LiVCrP2(O4F)2 (mp-767689) | 0.4429 | 0.186 | 6 |
LiMnVP2(O4F)2 (mp-778336) | 0.4561 | 0.001 | 6 |
LiVFeP2(O4F)2 (mp-777635) | 0.4419 | 0.026 | 6 |
LiVCrP2(O4F)2 (mp-868574) | 0.4426 | 0.006 | 6 |
LiVCrP2(O4F)2 (mp-765118) | 0.4549 | 0.111 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6701 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-6.8895 eV |
Corrected Energy-556.1446 eV
Uncorrected energy = -509.8246 eV
Composition-based energy adjustment (-0.687 eV/atom x 48.0 atoms) = -32.9760 eV
Composition-based energy adjustment (-1.668 eV/atom x 8.0 atoms) = -13.3440 eV
Corrected energy = -556.1446 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)