Final Magnetic Moment13.999 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.169 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.516 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiO8 + Li2FeO3 + Fe2NiO4 + LiFeO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 -1> | 107.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 121.8 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 142.7 |
CeO2 (mp-20194) | <1 0 0> | <1 -1 1> | 143.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 99.7 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 141.3 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 213.2 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 215.9 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 235.9 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 176.6 |
AlN (mp-661) | <1 1 0> | <0 1 -1> | 216.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 213.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 91.4 |
SiO2 (mp-6930) | <1 1 0> | <1 -1 1> | 143.0 |
SiO2 (mp-6930) | <1 1 1> | <1 -1 1> | 250.3 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 317.9 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 317.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 99.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 212.0 |
GaN (mp-804) | <0 0 1> | <1 1 -1> | 151.2 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 178.4 |
GaN (mp-804) | <1 0 1> | <1 1 -1> | 151.2 |
GaN (mp-804) | <1 1 1> | <1 1 -1> | 151.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 317.9 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 185.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 274.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 213.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 141.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 176.6 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 107.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 274.1 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 233.0 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 141.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 141.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 199.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 365.4 |
CdS (mp-672) | <0 0 1> | <1 -1 1> | 178.8 |
CdS (mp-672) | <1 0 0> | <1 -1 1> | 178.8 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 233.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 152.3 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 70.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 30.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 199.4 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 157.3 |
Te2W (mp-22693) | <0 1 1> | <1 -1 1> | 286.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 152.3 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 291.2 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 176.6 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 213.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 107.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(NiO2)2 (mp-762255) | 0.2240 | 0.050 | 3 |
MgMn2O4 (mp-1097894) | 0.1944 | 0.072 | 3 |
Ca(MnS2)2 (mvc-16788) | 0.1569 | 0.092 | 3 |
LiCr2O4 (mvc-16816) | 0.2212 | 0.237 | 3 |
MgMn2O4 (mp-1002568) | 0.1815 | 0.072 | 3 |
Li2Cr3FeO8 (mp-780014) | 0.1692 | 0.662 | 4 |
Li2FeCo3O8 (mp-763922) | 0.1944 | 0.095 | 4 |
Li2Cr3CoO8 (mp-763336) | 0.1888 | 0.081 | 4 |
Li2MnFe3O8 (mp-768068) | 0.1845 | 0.090 | 4 |
Li2Fe3CoO8 (mp-762906) | 0.1893 | 0.064 | 4 |
Ni3O4 (mp-714961) | 0.2487 | 0.000 | 2 |
Fe3O4 (mp-715614) | 0.3083 | 0.468 | 2 |
Fe3O4 (mp-612405) | 0.3246 | 0.177 | 2 |
Ni3O4 (mp-656887) | 0.2551 | 0.000 | 2 |
Ni3O4 (mp-849536) | 0.3700 | 0.130 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Ni_pv O |
Final Energy/Atom-5.3557 eV |
Corrected Energy-90.9612 eV
-90.9612 eV = -74.9799 eV (uncorrected energy) - 10.3630 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)