Final Magnetic Moment0.172 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.207 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.178 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.40 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiO8 + Fe2NiO4 + Li(NiO2)2 + Li2NiO3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 -1> | 240.9 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 192.7 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 296.2 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 197.4 |
CeO2 (mp-20194) | <1 0 0> | <1 1 -1> | 275.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 1> | 95.8 |
AlN (mp-661) | <1 0 0> | <1 1 -1> | 206.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 33.5 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 144.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 201.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 58.4 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 287.5 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 246.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 175.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 301.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 148.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 -1> | 96.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 1> | 95.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 191.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 -1> | 138.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 164.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 301.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 33.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 116.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 33.5 |
ZnSe (mp-1190) | <1 1 0> | <1 1 1> | 95.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 167.7 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 268.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 58.4 |
CdS (mp-672) | <0 0 1> | <1 0 -1> | 240.9 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 201.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 33.5 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 95.8 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 152.9 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 246.5 |
TePb (mp-19717) | <1 1 0> | <1 1 1> | 191.7 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 48.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 301.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 33.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 58.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 119.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 175.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 175.2 |
BN (mp-984) | <1 1 1> | <1 0 -1> | 337.3 |
BN (mp-984) | <1 0 1> | <1 0 -1> | 144.6 |
BN (mp-984) | <1 1 0> | <0 0 1> | 233.6 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 148.1 |
LiNbO3 (mp-3731) | <1 0 1> | <1 1 0> | 298.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 -1> | 240.9 |
Bi2Se3 (mp-541837) | <1 0 0> | <0 1 0> | 246.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(NiO2)2 (mp-762255) | 0.1734 | 0.050 | 3 |
MgMn2O4 (mp-1097894) | 0.1934 | 0.072 | 3 |
Ca(MnS2)2 (mvc-16788) | 0.2092 | 0.092 | 3 |
LiCr2O4 (mvc-16816) | 0.2415 | 0.237 | 3 |
MgMn2O4 (mp-1002568) | 0.1901 | 0.072 | 3 |
Li2TiV3O8 (mp-769560) | 0.1819 | 0.065 | 4 |
Li2Cr3FeO8 (mp-780014) | 0.1763 | 0.671 | 4 |
Li2Cr3FeO8 (mp-779991) | 0.1799 | 0.644 | 4 |
LiCoNiO4 (mp-763751) | 0.1758 | 0.057 | 4 |
Li2MnFe3O8 (mp-768068) | 0.1600 | 0.090 | 4 |
Ni3O4 (mp-714961) | 0.2674 | 0.000 | 2 |
Fe3O4 (mp-715614) | 0.3925 | 0.468 | 2 |
Fe3O4 (mp-612405) | 0.4113 | 0.876 | 2 |
Ni3O4 (mp-656887) | 0.2723 | 0.000 | 2 |
Ni3O4 (mp-849536) | 0.4074 | 0.130 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Ni_pv O |
Final Energy/Atom-5.0168 eV |
Corrected Energy-85.6101 eV
Uncorrected energy = -70.2351 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Composition-based energy adjustment (-2.256 eV/atom x 1.0 atoms) = -2.2560 eV
Composition-based energy adjustment (-2.541 eV/atom x 3.0 atoms) = -7.6230 eV
Corrected energy = -85.6101 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)