Final Magnetic Moment2.826 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.169 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.182 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.79 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa5Mn2P2(CO7)2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 288.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 210.3 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 288.3 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 113.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 180.1 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 118.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 300.2 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 278.7 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 113.3 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 288.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 210.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 240.2 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 288.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 300.2 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 278.7 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 300.2 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 60.0 |
TePb (mp-19717) | <1 1 1> | <0 1 0> | 288.3 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 278.7 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 120.1 |
BN (mp-984) | <0 0 1> | <1 0 0> | 280.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 300.2 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 300.2 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 180.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 240.2 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 185.8 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 300.2 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 0> | 288.3 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 226.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 60.0 |
C (mp-66) | <1 0 0> | <0 1 0> | 192.2 |
C (mp-66) | <1 1 0> | <0 1 0> | 288.3 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 210.3 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 0 0> | 140.2 |
LaF3 (mp-905) | <1 0 1> | <0 1 0> | 288.3 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 278.7 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 240.2 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 210.3 |
Ga2O3 (mp-886) | <1 0 -1> | <0 1 1> | 113.3 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 288.3 |
WS2 (mp-224) | <1 0 1> | <0 1 1> | 226.6 |
C (mp-48) | <0 0 1> | <1 0 1> | 278.7 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 300.2 |
ZrO2 (mp-2858) | <1 0 -1> | <0 1 0> | 288.3 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 288.3 |
YAlO3 (mp-3792) | <0 0 1> | <0 1 0> | 288.3 |
YAlO3 (mp-3792) | <0 1 1> | <0 1 0> | 96.1 |
YAlO3 (mp-3792) | <1 0 1> | <0 1 0> | 96.1 |
YAlO3 (mp-3792) | <1 1 1> | <0 1 0> | 192.2 |
TiO2 (mp-390) | <0 0 1> | <0 1 0> | 288.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3Ca(BO2)5 (mp-542719) | 0.6703 | 0.000 | 4 |
LiSn10(PO4)7 (mp-765193) | 0.6888 | 0.086 | 4 |
Ba2Zn(BO3)2 (mp-559138) | 0.7432 | 0.000 | 4 |
Na5Mn2P2(CO7)2 (mp-770045) | 0.3075 | 0.013 | 5 |
Na5Mn2P2(CO7)2 (mp-769536) | 0.2576 | 0.153 | 5 |
Na5Mn2P2(CO7)2 (mp-769529) | 0.2990 | 0.005 | 5 |
Na5Mn2P2(CO7)2 (mp-769465) | 0.2032 | 0.002 | 5 |
Na5Mn2P2(CO7)2 (mp-769461) | 0.2688 | 0.007 | 5 |
Na2LiMnPCO7 (mp-773710) | 0.3415 | 0.027 | 6 |
Na2LiFePCO7 (mp-773678) | 0.3493 | 0.132 | 6 |
Na5LiFe2P2(CO7)2 (mp-773523) | 0.3561 | 0.148 | 6 |
Na2LiFePCO7 (mp-773940) | 0.3554 | 0.099 | 6 |
Na5LiMn2P2(CO7)2 (mp-773342) | 0.3577 | 0.116 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Na_pv Mn_pv P C O |
Final Energy/Atom-6.5787 eV |
Corrected Energy-355.3216 eV
-355.3216 eV = -328.9341 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)